MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type 316L Stainless Steel, annealed and cold drawn bar
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Similar to Type 316 for superior corrosion resistance, but also has superior resistance to intergranular corrosion following welding or stress relieving. Good corrosion resistance to most chemicals, salts, and acids and molybdenum content helps resistance to marine environments. The low carbon content of 316L reduces the possibility of in vivo corrosion for medical implant use. High creep strength at elevated temperatures. 316L has fabrication characteristics similar to Types 302 and 304.

Applications: biomedical implants, chemical processing, food processing, photographic, pharmaceutical, textile finishing, marine exterior trim.

Key Words: UNS S31603, AISI 316L, ISO 2604-1 F59, ISO 2604-4 P57, ISO 2604-4 P58, ISO 4954 X2CrNiMo17133E, ISO 683/13 19, ISO 683/13 19a, biomaterials, biomedical implants, biocompatible materials
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 190190
Hardness, Knoop 212212Converted from Brinell
Hardness, Rockwell B 9191
Hardness, Vickers 199199Converted from Brinell
Tensile Strength, Ultimate 585 MPa84800 psi
Tensile Strength, Yield 380 MPa55100 psi
Elongation at Break 45 %45 %in 50 mm
Tensile Modulus 193 GPa28000 ksi
Izod Impact 150 J111 ft-lb21ºC
Charpy Impact 103 J76.0 ft-lbV-notch, 30ºC
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000740 ohm-cm0.0000740 ohm-cmat 20ºC
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 14.0 - 15.9 W/m-K97.0 - 110 BTU-in/hr-ft²-°F
Melting Point 1375 - 1400 °C2507 - 2550 °F
Solidus 1375 °C2507 °F
Liquidus 1400 °C2550 °F
Maximum Service Temperature, Air 870 °C1600 °FIntermittent
 925 °C1700 °FContinuous Service
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 61.9 - 72 %61.9 - 72 %As Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %2.0 - 3.0 %
Nickel, Ni 10 - 14 %10 - 14 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 316L Stainless Steel, annealed bar
AISI Type 316L Stainless Steel, annealed plate
AISI Type 316L Stainless Steel, annealed sheet
AISI Type 316L Stainless Steel, annealed strip
316 Stainless Steel, annealed and cold drawn bar

MQ316R / 12805

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.