MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Marfak® 0
Categories: Fluid; Lubricant; Organic Soap Gellant

Material Notes: Texaco Marfak grease delivers value through:
  • Good film strength
  • Good rust and corrosion protection, even in wet conditions.

Texaco Marfak greases are fibrous sodium soap greases. It resists oil separation and protects against dirt and rust. Texaco Marfak grease is formulated to:

  • Protect equipment from dust and dirt by providing a seal
  • Protect equipment against rusting in the presence of small amounts of water.

Texaco Marfak greases are recommended for slow speed, plain bearing and general-purpose lubrication of agricultural equipment.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 220927; MSDS Number: 9003

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Saybolt Viscosity at 100°F 4853 SUS4853 SUSSee Note 3.
Saybolt Viscosity at 210°F 181 SUS181 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 880 cSt880 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 37 cSt37 cStSee Note 3.
 
Mechanical PropertiesMetricEnglishComments
Penetration P(60), 1/10 mm 370370Unknown Amount of Work, 25°C (77°F)
Oil Separation 1.7 %1.7 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °FSee Note 2.
Minimum Service Temperature, Air -12.0 °C10.4 °FSee Note 1.
Flash Point 220 °C428 °FSee Note 3.
Dropping Point 166 °C331 °F
 
Descriptive Properties
ColorDark Brown
Rust PreventionPass
TextureStringy
Thickener, %7Sodium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Marfak® Heavy Duty 2
ChevronTexaco Novatex® EP NLGI Grade 1
ChevronTexaco Novatex® EP NLGI Grade 000
ChevronTexaco Thuban® SAE 80W-90
ChevronTexaco Thuban® SAE 250

WTEXA247 / 77126

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.