MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eagle Brass 316L Austenitic Stainless Steel, 1/8 Hardened
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical and photographic equipment, valve and pump trim, chemical equipment, digesters, tanks, evaporators, pulp, paper and textile processing equipment and parts exposed to marine atmospheres and tubing.

Information provided by Eagle Brass Company

Key Words: ASTM A666; UNS S31603
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.92 g/cc0.286 lb/in³As Annealed
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 689 MPa>= 100000 psi
Tensile Strength, Yield >= 379 MPa>= 55000 psi0.2% Offset
Elongation at Break >= 30 %>= 30 %in 2 inches
Tensile Modulus 193 GPa28000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.5 µm/m-°C
@Temperature 20.0 - 649 °C
10.3 µin/in-°F
@Temperature 68.0 - 1200 °F
Thermal Conductivity 15.9 W/m-K110 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 62.145 - 72 %62.145 - 72 %Calculated as Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %2.0 - 3.0 %
Nickel, Ni 10 - 14 %10 - 14 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eagle Brass 316L Austenitic Stainless Steel, Annealed
Greene Tweed CHEMRAZ® 510 Perfluoroelastomer
Greene Tweed CHEMRAZ® 526 Perfluoroelastomer
Greene Tweed CHEMRAZ® 615 Perfluoroelastomer
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C)

NEAGLE544 / 147521

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.