MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HD 7845.30 MMW Blown Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides excellent film appearance and high quality recycle. HD 7845.30 is particularly recommended as a blend component with LLDPE for stiff clear films.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Deli Wrap
  • Food packaging
  • Heavy Duty Bags
  • Oriented Film Products
  • Overwrap Film
  • Surface Protection Film
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.958 g/cc0.0346 lb/in³ExxonMobil Method
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
30 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 34.5 MPa5000 psiASTM D882
Film Tensile Strength at Yield, TD 13.1 MPa1900 psiASTM D882
Film Elongation at Break, MD 420 %420 %ASTM D882
Film Elongation at Break, TD 4.0 %4.0 %ASTM D882
Elmendorf Tear Strength, MD 0.354 g/micron9.00 g/milASTM D1922
Elmendorf Tear Strength, TD 30.7 g/micron780 g/milASTM D1922
Dart Drop >= 1.57 g/micron>= 40.0 g/milASTM D1709
Film Tensile Strength at Break, MD 82.7 MPa12000 psiASTM D882
Film Tensile Strength at Break, TD 36.5 MPa5300 psiASTM D882
1% Secant Modulus, MD 1100 MPa160000 psiASTM D882
1% Secant Modulus, TD 1590 MPa230000 psiASTM D882
 
Descriptive Properties
FeaturesThermal Stabilizer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 9605D HDPE Cast Film Resin
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
ExxonMobil HD 5805 High Density Polyethylene Resin
ExxonMobil HD 7960.13 HMW Blown Film Resin
BCC Products DP-11-83 Urethane Adhesive-Slo

PEXB074 / 37379

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.