MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chengdu Polyster H605 Thermoplastic Polyether-ester Elastomer (TPEE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyether Ester Elastomer

Material Notes: Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent tear resistance. Molded and injected products for consumer use, such as airbag door covers, railway tie pads, seals, wires, cables and optical fiber.

Information provided by Chengdu Polyster Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Melt Flow 6.0 - 8.0 g/10 min6.0 - 8.0 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ISO 868
Tensile Strength, Ultimate 35.0 MPa5080 psiISO 527-1
Elongation at Break 500 %500 %ISO 527-1
Flexural Modulus 0.206 GPa29.9 ksiISO 178
Tear Strength 153 kN/m873 pliISO 34
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 °C392 °FISO 3146
Brittleness Temperature -70.0 °C-94.0 °FISO 974

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chengdu Polyster H3303 Thermoplastic Polyether-ester Elastomer (TPEE)
Samyang Triel® 5700(A) Thermoplastic Polyether Ester Elastomer
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer
Chengdu Polyster FH3303 Thermoplastic Polyether-ester Elastomer (TPEE)
EMS-Grivory Grilamid® L 20 LM PA12

PCHEN035 / 79332

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.