MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lushan EV1050G1/RF EVA Film for Encapsulating Solar modules, Reinforced Friendly
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemical Accessories. EVA film for encapsulating solar modules Lushan series could effectively protect to the PV cell, and has excellent performance of transmittance and ageing-resistant. It provides structural support, electrical isolation, physical isolation/protection, and thermal conduction for solar circuits, as well as to maximize the service life of solar module. Solar EVA Film Characteristic:
  • High volume resistivity and lasting adhesion strength holding capacity, and insure PV modules have long service life
  • Low yellowness index change and low light transmittance attenuation, insure the high service efficiency of PV modules
  • Excellent compatibility with flux, welding ribbon, location tap, backsheet and silica gel
  • Solar EVA film quality stability ensured by the complete and scientific quality management system.

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ISO 1183
Water Absorption <= 0.10 %<= 0.10 %ISO 62:2008
Melt Flow 17 - 27 g/10 min17 - 27 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.0 MPa2180 psiISO 527-3
Elongation at Break >= 400 %>= 400 %
Tensile Modulus 0.00800 GPa1.16 ksiYoung's; ISO 527-3
Peel Strength  0.00120 kN/m
@Time 0.000 sec
0.00685 pli
@Time 0.000 hour
180° peel, peel speed is 100 mm/min
 0.00125 kN/m
@Time 1.44e+6 sec
0.00713 pli
@Time 400 hour
180° peel, peel speed is 100 mm/min
 0.00132 kN/m
@Time 2.88e+6 sec
0.00753 pli
@Time 800 hour
180° peel, peel speed is 100 mm/min
 0.00150 kN/m
@Time 3.24e+6 sec
0.00856 pli
@Time 900 hour
180° peel, peel speed is 100 mm/min
 0.00153 kN/m
@Time 7.20e+6 sec
0.00873 pli
@Time 2000 hour
180° peel, peel speed is 100 mm/min
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 65.0 - 75.0 °C149 - 167 °FASTM D148
Shrinkage, MD 0.00 %
@Temperature 120 °C,
Time 180 sec
0.00 %
@Temperature 248 °F,
Time 0.0500 hour
Q/LSXC
Shrinkage, TD 0.00 %
@Temperature 120 °C,
Time 180 sec
0.00 %
@Temperature 248 °F,
Time 0.0500 hour
Q/LSXC
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ISO 489
Yellow Index  2.9 %
@Time 0.000 sec
2.9 %
@Time 0.000 hour
 3.0 %
@Time 0.000 sec
3.0 %
@Time 0.000 hour
after heat and humidity aging (85°c, 85 RH%)
 3.5 %
@Time 3.60e+6 sec
3.5 %
@Time 1000 hour
after heat and humidity aging (85°c, 85 RH%)
 3.9 %
@Time 3.60e+6 sec
3.9 %
@Time 1000 hour
 4.0 %
@Time 5.40e+6 sec
4.0 %
@Time 1500 hour
 4.9 %
@Time 7.20e+6 sec
4.9 %
@Time 2000 hour
 5.0 %
@Time 7.20e+6 sec
5.0 %
@Time 2000 hour
after heat and humidity aging (85°c, 85 RH%)
 
Descriptive Properties
Surface UncuredOne Side Embossed
Thickness Tolerance±0.02Q/LSXC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvax® 440 Ethylene Vinyl Acetate
Dow Elvax® 3134SBZ Ethylene Vinyl Acetate
ExxonMobil Escorene® LD 713.93 Cast Film Resin
ExxonMobil EXACT™ 4150 Plastomer
Dow Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film

PLUSH013 / 150011

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.