MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primer

Recommended Primers: Dow Corning S2260

Design/Construction:
Liner: FEP
Product: Uncured Silicone Rubber
Carrier: PTFE Coated Fiberglass

Appearance: White silicone gum

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns1.00 milLiner
 76.2 microns3.00 milCarrier
 203 microns8.00 milOverall; Arlon SQA-TMS-003
Outgassing - Total Mass Loss 0.30 %0.30 %Arlon SQA-TMS-045
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585Silicone Property; ASTM D2240
Tensile Strength 2.07 MPa300 psiSilicone Property; ASTM D412
Elongation at Break 28 %28 %Silicone Property; ASTM D412
Modulus of Elasticity 0.0328 GPa4.75 ksiASTM E 831
Poissons Ratio 0.500.50Approximately, Silicone Property
Shear Strength 1.28 MPa185 psiLap Shear Strength; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
Dk, Silicone Property; IPC TM 650-2.5.5.3
Dielectric Strength 37.4 kV/mm950 kV/inASTM D149
Dissipation Factor 0.0028
@Frequency 1e+6 Hz
0.0028
@Frequency 1e+6 Hz
Df, Silicone Property; IPC TM 650-2.5.5.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 39.0 µm/m-°C21.7 µin/in-°FSilicone Property; ASTM E 831
Specific Heat Capacity 0.700 J/g-°C0.167 BTU/lb-°FE 1461-01
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°FSilicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg -110 - -95.0 °C-166 - -139 °FSilicone Property; ASTM D3418
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 121 °C
0.250 hour
@Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
6.00 Month
@Temperature 40.0 - 50.0 °F
From date of manufacture
 
Descriptive Properties
ColorBlue
Total Product Weight (g/m2)345Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adamas Adalon® 413 PTFE, 20% PPS
Epoxy Technology EPO-TEK® TV2001 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® T7109-17 Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy
Epoxy Technology EPO-TEK® ED1021 Epoxy

PARL645 / 125831

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.