MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 4414 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Flock Filled

Material Notes: PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional stability. UL recognized under component file E40654. 04414 is available in black.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 g/cc0.0224 lb/in³ASTM D1895
Density 1.54 g/cc0.0556 lb/in³ASTM D792
Water Absorption 0.26 %0.26 %ASTM D570
Linear Mold Shrinkage 0.0068 cm/cm0.0068 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7979ASTM D785
Tensile Strength, Ultimate 53.0 MPa7690 psiASTM D638
Elongation at Break 0.77 %0.77 %ASTM D638
Tensile Modulus 10.1 GPa1460 ksiASTM D638
Flexural Strength 82.0 MPa11900 psiASTM D790
Flexural Modulus 8.00 GPa1160 ksiASTM D790
Compressive Strength 177 MPa25700 psiASTM D695
Izod Impact, Notched 0.166 J/cm0.311 ft-lb/inASTM D256
Charpy Impact, Notched 0.203 J/cm²0.966 ft-lb/in²ASTM D256
Impact 118118J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.40e+11 ohm-cm8.40e+11 ohm-cmASTM D247
Dielectric Constant 5.35.3ASTM D150
Dielectric Strength 12.5 kV/mm318 kV/inShort Time; ASTM D149
Dissipation Factor 0.0510.051ASTM D150
Arc Resistance 151 sec151 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 168 °C334 °FASTM D648
Flammability, UL94 V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
Shrinkage 0.24 %0.24 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 4414 Phenolic, Granular, Transfer Molded
Plenco 2000 Phenolic, Granular, Transfer Molded
Plenco 2000 Phenolic, Granular, Injection Molded
Plenco 2308 Phenolic, Granular, Transfer Molded
Plenco 2308 Phenolic, Granular, Injection Molded

PLEL83d / 50656

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.