MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SMAC SMACMOUNT® 1195S Damping Material
Categories: Other Engineering Material

Material Notes: Specifications - Shock & vibration insulation for:
  • Embedded electronic
  • Trays & racks systems
Advantages:
  • No special tools required
  • High damping isolators
  • Small Size

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °FSMACTANE®
 150 °C302 °FSMACSIL®
Minimum Service Temperature, Air -55.0 °C-67.0 °FSMACSIL®
 -30.0 °C-22.0 °FSMACTANE®
 
Descriptive Properties
Frequency100-140 Hz
Load2.2 - 6.6 lbs
MaterialsSMACSIL®
 SMACTANE®
Metal partsStainless steel
Overall size13 mmø ext.
 27 mmHeight
Transmissibility at resonance<2.5SMACTANE®
 <4SMACSIL®
Weight2.5 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 4014 Damping Aluminum Foam Sheet
3M 2552 Damping Foil
SMAC BARRIER® Damping Material
304 Stainless Steel
Overview of materials for Acrylic, General Purpose, Molded

PZSMAC017 / 146133

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.