MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1095 Steel, oil quenched 800°C (1470°F), 480°C (900°F) temper, 25 mm (1 in.) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; High Carbon Steel

Material Notes: Applications include edge tools, wear-resistant parts, high-stress flat springs, hot coiled springs, plow beams, plow shares, scraper blades, discs, mower knives, and harrow teeth. Post oil quenched hardness: 46 HRC surface, 42 HRC half-radius, 40 HRC center

Key Words: UNS G10950, AMS 5121, AMS 5122, AMS 5132, AMS 7304, ASTM A29, ASTM A510, ASTM A576, ASTM A682, FED QQ-S-700 (C1095), MIL SPEC MIL-S-16788 (C10), SAE J403, SAE J412, SAE J414, DIN 1.1274, JIS SUP 4, SS14 1870 (Sweden), B.S. 060 A 96, B.S. EN 44 B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steel.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 352352
Hardness, Knoop 381381Converted from Brinell
Hardness, Rockwell B 9999Converted from Brinell
Hardness, Rockwell C 3939Converted from Brinell
Hardness, Vickers 372372Converted from Brinell
Tensile Strength, Ultimate 1215 MPa176200 psi
Tensile Strength, Yield 703 MPa102000 psi
Elongation at Break 10 %10 %in 50 mm
Reduction of Area 23.4 %23.4 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel.
Izod Impact 3.00 J2.21 ft-lbannealed at 790°C (1450°F)
 4.00 J2.95 ft-lbas rolled
 5.00 J3.69 ft-lbnormalized at 900°C (1650°F)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000180 ohm-cm
@Temperature 20.0 °C
0.0000180 ohm-cm
@Temperature 68.0 °F
condition of specimen unknown
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 0.000 - 100 °C
6.11 µin/in-°F
@Temperature 32.0 - 212 °F
 11.7 µm/m-°C
@Temperature 0.000 - 200 °C
6.50 µin/in-°F
@Temperature 32.0 - 392 °F
 12.4 µm/m-°C
@Temperature 0.000 - 300 °C
6.89 µin/in-°F
@Temperature 32.0 - 572 °F
 13.1 µm/m-°C
@Temperature 0.000 - 400 °C
7.28 µin/in-°F
@Temperature 32.0 - 752 °F
 13.5 µm/m-°C
@Temperature 0.000 - 500 °C
7.50 µin/in-°F
@Temperature 32.0 - 932 °F
 14.2 µm/m-°C
@Temperature 0.000 - 600 °C
7.89 µin/in-°F
@Temperature 32.0 - 1110 °F
 14.6 µm/m-°C
@Temperature 0.000 - 700 °C
8.11 µin/in-°F
@Temperature 32.0 - 1290 °F
Specific Heat Capacity 0.461 J/g-°C
@Temperature >=100 °C
0.110 BTU/lb-°F
@Temperature >=212 °F
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.90 - 1.03 %0.90 - 1.03 %
Iron, Fe 98.38 - 98.8 %98.38 - 98.8 %As remainder
Manganese, Mn 0.30 - 0.50 %0.30 - 0.50 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1095 Steel, oil quenched from 800°C (1475°F), tempered at 480°C (900°F)
AISI 1095 Steel, normalized at 900°C (1650°F), air cooled, 13 mm (0.5 in.) round
AISI 1095 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1095 Steel, as rolled
AISI 1095 Steel, normalized at 900°C (1650°F), air cooled, 25 mm (1 in.) round

M1095O / 7114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.