MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ecoflex® F BX 7011 Biodegradable Plastic
Categories: Polymer; Film; Renewable/Recycled Polymer

Material Notes: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex F BX 7011 comes closer than any other biodegradable plastic to the processing properties of LDPE and LLDPE. Blown film extrusion is a particular area where Ecoflex F shows well-balanced processing properties, and the resin can also be used in extrusion coating applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 - 1.27 g/cc0.0452 - 0.0459 lb/in³ISO 1183
Moisture Vapor Transmission 140 cc-mm/m²-24hr-atm356 cc-mil/100 in²-24hr-atm100% RH; ASTM Test
Oxygen Transmission Rate 1600 cc/m²/day103 cc/100 in²/day0% RH; ASTM Test
Melt Flow 2.7 - 4.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.7 - 4.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Yield, MD 560 %560 %ASTM Data
Film Elongation at Yield, TD 700 %700 %ASTM Data
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 120 °C230 - 248 °F10 K/min
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 82 %82 %
 
Descriptive Properties
ColorTransparent
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueBlown Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ecoflex® C1200 F Blend Biodegradable Polyester
BASF Ecoflex® 1200 F Blend Biodegradable Polyester
BASF Ecoflex® P BX 7020 Biodegradable Polyester
BASF Ecovio® C2203 F Blend Biodegradable Polyester
BASF Ecovio® C2224 F Blend Biodegradable Polyester

PBASF9000 / 84764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.