MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: VE-0856U is the UV-Stabilized Version.

Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 33 g/10 min
@Load 10.0 kg,
Temperature 220 °C
33 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9797ASTM D785
Tensile Strength, Yield 39.3 MPa
@Thickness 3.17 mm
5700 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 15 %
@Thickness 3.17 mm
15 %
@Thickness 0.125 in
ASTM D638
Flexural Strength 55.2 MPa
@Thickness 3.17 mm
8000 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.28 GPa
@Thickness 3.17 mm
330 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched  1.76 J/cm
@Thickness 6.35 mm
3.30 ft-lb/in
@Thickness 0.250 in
ASTM D256
 2.46 J/cm
@Thickness 3.17 mm
4.60 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.9 °C
@Thickness 6.35 mm
174 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 90.0 °C194 °FUnannealed; ISO R 306
Flammability, UL94 5VB5VBUL94
 5VA5VAUL94
 V-0
@Thickness 2.50 mm
V-0
@Thickness 0.0984 in
UL94
 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
UL94
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL94
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 180 °C338 - 356 °F
Middle Barrel Temperature 190 - 200 °C374 - 392 °F
Front Barrel Temperature 200 - 210 °C392 - 410 °F
Melt Temperature 210 - 220 °C410 - 428 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 58.80 - 108 MPa8528 - 15600 psi
Back Pressure 0.689 - 1.38 MPa100 - 200 psi
Screw Speed 50 - 70 rpm50 - 70 rpm
 
Descriptive Properties
UV Resistance<3 Delta E300 Hr. Ivory Color; ASTM D4459

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® VE-0856 G ABS
Chi Mei Polylac® PA-765 ABS - Flame Retardant
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
TPI Porene® ABS-SP-100 Super High Impact ABS Resin
Chi Mei Polylac® PA-757 ABS

PLBST005 / 50490

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.