MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iran Petrochemical (PCC) X 30 G Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: X30G is for injection molding because of its good flow properties this grade offers easy processing and extruded items exhibit high stiffness.

Applications: The grade is widely used for injection molding consumer goods such as feed containers, house wares, toys, garden furniture and parts for the automotive industry.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 9.0 g/10 min9.0 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7171ISO 868
Tensile Stress 34.0 MPa4930 psiISO R527
Elongation at Yield 13 %13 %ISO R527
Flexural Modulus 1.50 GPa218 ksiISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 155 °C311 °FISO 306/A
Heat Distortion Temperature 115 °C239 °FISO 75/B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) V 30 S Polypropylene
Iran Petrochemical (PCC) T 30 S Polypropylene
Iran Petrochemical (PCC) Moplen Z 30 S Polypropylene
Iran Petrochemical (PCC) Moplen Z 30 G Polypropylene
Iran Petrochemical (PCC) X 30 S Polypropylene Film

PIPC310 / 149744

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.