MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total HP 401 MDPE, pipe, cable, sheet
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process.

FINATHENE® HP 401 is a black high density polyethylene specially developed for applications where excellent properties and high stiffness and creep resistance are required (e.g. sewage and drainage pipes, industrial pipes, sheet for chemical storage vessels,.)

FINATHENE® HP 401 is a black high density polyethylene developed for cable sheathing applications and is designed to meet the requirements for communication power cables (medium and high voltage cable applications).

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ISO 1183
Environmental Stress Crack Resistance >= 700 hour>= 700 hourASTM D1693
Oxidative Induction Time (OIT) >= 20 min>= 20 min210°C; EN 728
 >= 30 min>= 30 min200°C; EN 728
Carbon Black Loading 2.0 - 2.5 %2.0 - 2.5 %ISO 6964
Melt Flow  0.10 g/10 min
@Load 2.16 kg
0.10 g/10 min
@Load 4.76 lb
ISO 1133
 0.52 g/10 min
@Load 5.00 kg
0.52 g/10 min
@Load 11.0 lb
ISO 1133
High Load Melt Index 10 g/10 min
@Load 21.6 kg
10 g/10 min
@Load 47.6 lb
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363DIN 53505
Tensile Strength at Break 34.0 MPa4930 psiISO 527
Tensile Strength, Yield 24.0 MPa3480 psiISO 527
Elongation at Break >= 700 %>= 700 %ISO 527
Elongation at Yield 9.0 %9.0 %ISO 527
Modulus of Elasticity 1.05 GPa152 ksiISO 178
Flexural Modulus 1.00 GPa145 ksiASTM D 790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 93
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmIEC 93
Dielectric Constant 2.35
@Frequency 1000 Hz
2.35
@Frequency 1000 Hz
IEC 250
Dielectric Strength 17.0 kV/mm432 kV/inIEC 243
Dissipation Factor  0.00020
@Frequency 1000 Hz
0.00020
@Frequency 1000 Hz
IEC 250
 0.00030
@Frequency 1e+6 Hz
0.00030
@Frequency 1e+6 Hz
IEC 250
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 175 J/g75.3 BTU/lbDSC
CTE, linear 160 µm/m-°C
@Temperature 20.0 °C
88.9 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 2.00 J/g-°C0.478 BTU/lb-°FDSC
 2.60 J/g-°C
@Temperature 150 °C
0.621 BTU/lb-°F
@Temperature 302 °F
DSC
Thermal Conductivity 0.200 W/m-K
@Temperature 150 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 302 °F
DIN 52612
Vicat Softening Point 127 °C261 °FISO 306
Brittleness Temperature -100 °C-148 °FASTM D 746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin
Total Xsene® XS10 BRS HDPE, pipe
Versalis Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin
LyondellBasell Alathon® L4903 High Density Polyethylene

PFINAP080 / 38663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.