MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nordic Grafting Company Acti-Tech™ 11MA13 Compatibilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Acti-Tech compatibilizers are based on Vistamaxx™ performance polymers grafted with maleic anhydride through a highly efficient melt-grafting process. Acti-Tech compatibilizer 11MA13 is a medium flexibility, low MFR grade among the Acti-Tech compatibilizers range. With its high viscosity, it is designed to enhance performance of a wide variety of polymer compounds and is particularly recommended for the following applications:
  • Tie-layer material for film & sheet
  • Adhesion promoter on metal, yarns or other polar substrates
  • Soft compatibilizer for polar/unpolar polymers alloys
  • Impact modifier of stiff polar engineering plastics
Due to the chemical nature of its polymer backbone, Acti-Tech compatibilizer 11MA13 is compatible with most polyolefins, i.e. PE, PP, EVA, EBA or POE.

Information provided by Nordic Grafting Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.0650 GPa9.43 ksiISO 178
 
Descriptive Properties
Maleic anhydride content>1.0%FTIR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gabriel Phenoxy™ PKHH Solid Polyhydroxylether
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer
VICTREX™ PEEK 381G Medium Viscosity
Resinlab® CYNERGY CA6001 Adhesive
Nordic Grafting Company Acti-Tech™ 08MA18 Compatibilizer

PNGC004 / 238946

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.