MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® 329S Polyester Film, 92 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: An opaque white film with good handling properties, a unique glossy appearance, and a lower shrinkage for special applications

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.396 g/cc0.05043 lb/in³ASTM D1505
Thickness 23.4 microns0.920 mil
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 82.7 MPa12000 psiASTM D882A
Film Tensile Strength at Yield, TD 82.7 MPa12000 psiASTM D882A
Film Elongation at Break, MD 115 %115 %ASTM D882A
Film Elongation at Break, TD 90 %90 %ASTM D882A
Film Tensile Strength at Break, MD 152 MPa22000 psiASTM D882A
Film Tensile Strength at Break, TD 159 MPa23000 psiASTM D882A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 197 kV/mm5000 kV/inASTM D149
Dielectric Breakdown 4600 V4600 VASTM D149
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 2.8 %
@Temperature 190 °C,
Time 300 sec
2.8 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.4 %
@Temperature 190 °C,
Time 300 sec
1.4 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Gloss 40 %40 %45°; ASTM D1003
 45 %45 %60°; ASTM D1003
Transmission, Visible 23 %23 %TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 329 Polyester Film, 300 Gauge
DuPont Teijin Films Melinex® 331 Polyester Film, 700 Gauge
DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 329 Polyester Film, 1400 Gauge
DuPont Teijin Films Melinex® 329 Polyester Film, 1000 Gauge

PDTZ9043 / 139440

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.