MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell Spectra® 1000 Fiber
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Spectra® fiber 1000, the second in a series of Spectra® fibers, was developed to meet customers’ needs for increased performance. It is available in a multitude of deniers for use in a wide range of applications. This extended chain polyethylene fiber has one of the highest strength to weight ratios of any manmade fiber. Spectra® fiber 1000 has a tenacity 15 – 20 percent higher than that of Spectra® fiber 900. Spectra® fiber is, pound-for-pound, 10 times stronger than steel, more durable than polyester and has a specific strength that is 40 percent greater than aramid fiber. Specific performance is dependent upon denier and filament count.  Spectra® is a registered trademark of Honeywell and was formerly a product of Allied Signal.

Key Words: FRP composites, single fiber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3000 MPa435000 psi
Modulus of Elasticity 172 GPa24900 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 147 °C297 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell Spectra® 900 Fiber
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Toyobo Dyneema® SK60 High Strength Polyethylene Fiber
DuPont™ Kevlar® 29 Aramid Fiber

PCF007 / 27994

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.