MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1055 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; High Carbon Steel

Material Notes: Applications include battering tools, hot upset forging dies, ring-rolling tools, wear-resistant parts, hand tools, and parts for agricultural implements which require high strength at low cost. When heat treated, this steel yields a high surface hardness, combined with good toughness. Good forging characteristics.

Key Words: UNS G10550, ASTM A29, ASTM A510, ASTM A576, ASTM A682, FED QQ-S-700 (C1055), EN43C, SAE J403, SAE J412, SAE J414, DIN 1.1209
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steel.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 192192
Hardness, Knoop 214214Converted from Brinell
Hardness, Rockwell B 9191Converted from Brinell
Hardness, Rockwell C 1111Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 201201Converted from Brinell
Tensile Strength, Ultimate 650 MPa94300 psi
Tensile Strength, Yield 355 MPa51500 psi
Elongation at Break 12 %12 %
Reduction of Area 30 %30 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000163 ohm-cm
@Temperature 0.000 °C
0.0000163 ohm-cm
@Temperature 32.0 °F
condition of specimen unknown
 0.0000224 ohm-cm
@Temperature 100 °C
0.0000224 ohm-cm
@Temperature 212 °F
condition of specimen unknown
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 20.0 - 100 °C
6.11 µin/in-°F
@Temperature 68.0 - 212 °F
 12.1 µm/m-°C
@Temperature 20.0 - 200 °C
6.72 µin/in-°F
@Temperature 68.0 - 392 °F
 12.4 µm/m-°C
@Temperature 20.0 - 300 °C
6.89 µin/in-°F
@Temperature 68.0 - 572 °F
 13.3 µm/m-°C
@Temperature 20.0 - 400 °C
7.39 µin/in-°F
@Temperature 68.0 - 752 °F
 13.9 µm/m-°C
@Temperature 20.0 - 500 °C
7.72 µin/in-°F
@Temperature 68.0 - 932 °F
 14.4 µm/m-°C
@Temperature 20.0 - 600 °C
8.00 µin/in-°F
@Temperature 68.0 - 1110 °F
 14.8 µm/m-°C
@Temperature 20.0 - 700 °C
8.22 µin/in-°F
@Temperature 68.0 - 1290 °F
Specific Heat Capacity 0.472 J/g-°C0.113 BTU/lb-°FTypical steel
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.50 - 0.60 %0.50 - 0.60 %
Iron, Fe 98.41 - 98.9 %98.41 - 98.9 %As remainder
Manganese, Mn 0.60 - 0.90 %0.60 - 0.90 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1055 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1060 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1050 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1040 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

M1055B / 7005

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.