MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman ComAlloy Voloy® 110 Polypropylene, Mineral Reinforced, Flame Retardant, UL
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Data provided by the manufacturer, ComAlloy International Company.

15% Mineral Reinforced.

The ComAlloy product line has been integrated into the A Schulman product line.

Key Words: ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9898ASTM D785
Tensile Strength, Ultimate 30.0 MPa4350 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Flexural Strength 50.0 MPa7250 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched 0.430 J/cm0.806 ft-lb/inASTM D256
Izod Impact, Unnotched 7.10 J/cm13.3 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C244 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 210 - 221 °C410 - 430 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Global 110 Polypropylene
BASF Novolen® 1100 VC Polypropylene
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade

PASH2Y / 24869

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.