MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.

Benefits: The product offers an excellent long term heat resistance and is suitable to work in environments characterized by a very high temperature. It has been also specially designed to be perfectly suitable for blow molding processing.

Available in: Europe

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Thanks to its very high melt strength, this product can be used to produce hollow parts, by suction or 3D blow molding technology, like tanks or ducts where a long parison is needed. Typical applications are turbo air ducts, especially inlet ducts up to 210°C.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183/A
Viscosity  200 cP
@Shear Rate 1000 1/s,
Temperature 275 °C
200 cP
@Shear Rate 1000 1/s,
Temperature 527 °F
 1000 cP
@Shear Rate 100 1/s,
Temperature 275 °C
1000 cP
@Shear Rate 100 1/s,
Temperature 527 °F
 2000 cP
@Shear Rate 10 1/s,
Temperature 275 °C
2000 cP
@Shear Rate 10 1/s,
Temperature 527 °F
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inIsotropy
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psiISO 527 Type 1A
Tensile Stress at Strain  5.00 MPa
@Strain 1 %,
Temperature 200 °C
725 psi
@Strain 1 %,
Temperature 392 °F
 5.00 MPa
@Strain 1 %,
Temperature 230 °C
725 psi
@Strain 1 %,
Temperature 446 °F
 10.0 MPa
@Strain 2 %,
Temperature 230 °C
1450 psi
@Strain 2 %,
Temperature 446 °F
 12.0 MPa
@Strain 1 %,
Temperature 120 °C
1740 psi
@Strain 1 %,
Temperature 248 °F
 12.0 MPa
@Strain 1 %,
Temperature 160 °C
1740 psi
@Strain 1 %,
Temperature 320 °F
 12.0 MPa
@Strain 2 %,
Temperature 200 °C
1740 psi
@Strain 2 %,
Temperature 392 °F
 12.0 MPa
@Strain 3 %,
Temperature 230 °C
1740 psi
@Strain 3 %,
Temperature 446 °F
 15.0 MPa
@Strain 1 %,
Temperature 80.0 °C
2180 psi
@Strain 1 %,
Temperature 176 °F
 15.0 MPa
@Strain 6.0 %,
Temperature 230 °C
2180 psi
@Strain 6.0 %,
Temperature 446 °F
 19.0 MPa
@Strain 3 %,
Temperature 200 °C
2760 psi
@Strain 3 %,
Temperature 392 °F
 20.0 MPa
@Strain 2 %,
Temperature 160 °C
2900 psi
@Strain 2 %,
Temperature 320 °F
 20.0 MPa
@Strain 12 %,
Temperature 230 °C
2900 psi
@Strain 12 %,
Temperature 446 °F
 21.0 MPa
@Strain 3 %,
Temperature 160 °C
3050 psi
@Strain 3 %,
Temperature 320 °F
 21.0 MPa
@Strain 6.0 %,
Temperature 200 °C
3050 psi
@Strain 6.0 %,
Temperature 392 °F
 22.0 MPa
@Strain 2 %,
Temperature 120 °C
3190 psi
@Strain 2 %,
Temperature 248 °F
 25.0 MPa
@Strain 2 %,
Temperature 80.0 °C
3630 psi
@Strain 2 %,
Temperature 176 °F
 28.0 MPa
@Strain 6.0 %,
Temperature 160 °C
4060 psi
@Strain 6.0 %,
Temperature 320 °F
 30.0 MPa
@Strain 3 %,
Temperature 120 °C
4350 psi
@Strain 3 %,
Temperature 248 °F
 30.0 MPa
@Strain 12 %,
Temperature 200 °C
4350 psi
@Strain 12 %,
Temperature 392 °F
 32.0 MPa
@Strain 12 %,
Temperature 160 °C
4640 psi
@Strain 12 %,
Temperature 320 °F
 35.0 MPa
@Strain 1 %,
Temperature -40.0 °C
5080 psi
@Strain 1 %,
Temperature -40.0 °F
 35.0 MPa
@Strain 1 %,
Temperature 23.0 °C
5080 psi
@Strain 1 %,
Temperature 73.4 °F
 35.0 MPa
@Strain 3 %,
Temperature 80.0 °C
5080 psi
@Strain 3 %,
Temperature 176 °F
 40.0 MPa
@Strain 6.0 %,
Temperature 120 °C
5800 psi
@Strain 6.0 %,
Temperature 248 °F
 42.0 MPa
@Strain 12 %,
Temperature 120 °C
6090 psi
@Strain 12 %,
Temperature 248 °F
 45.0 MPa
@Strain 6.0 %,
Temperature 80.0 °C
6530 psi
@Strain 6.0 %,
Temperature 176 °F
 45.0 MPa
@Strain 12 %,
Temperature 80.0 °C
6530 psi
@Strain 12 %,
Temperature 176 °F
 75.0 MPa
@Strain 2 %,
Temperature 23.0 °C
10900 psi
@Strain 2 %,
Temperature 73.4 °F
 90.0 MPa
@Strain 2 %,
Temperature -40.0 °C
13100 psi
@Strain 2 %,
Temperature -40.0 °F
 90.0 MPa
@Strain 3 %,
Temperature 23.0 °C
13100 psi
@Strain 3 %,
Temperature 73.4 °F
 120 MPa
@Strain 3 %,
Temperature -40.0 °C
17400 psi
@Strain 3 %,
Temperature -40.0 °F
 140 MPa
@Strain 4 %,
Temperature -40.0 °C
20300 psi
@Strain 4 %,
Temperature -40.0 °F
Elongation at Break 4.7 %4.7 %ISO 527 Type 1A
Tensile Modulus 4.90 GPa711 ksiISO 527 Type 1A
Flexural Strength 129 MPa18700 psiISO 178
Flexural Modulus 4.20 GPa609 ksiISO 178
Charpy Impact Unnotched 6.50 J/cm²30.9 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.35 J/cm²6.42 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75/Af
 
Processing PropertiesMetricEnglishComments
Feed Temperature 265 - 285 °C509 - 545 °F
Adapter Temperature 275 - 295 °C527 - 563 °F
Die Temperature 280 - 300 °C536 - 572 °F
Head Temperature 280 - 300 °C536 - 572 °F
Screw Cooling Temperature 275 - 295 °C527 - 563 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C
@Time 28800 sec
176 °F
@Time 8.00 hour
dew point -35°C
Moisture Content <= 0.080 %<= 0.080 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 230 V13 PA66, 13% glass fiber, Conditioned
Domo TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY
Celanese Zytel® 70G30HSLR BK099 PA66-GF30
Domo TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY

PRHOD720 / 137951

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.