MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zenite® 9140HT NC010 LCP  (discontinued **)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled

Material Notes: Zenite® 9140HT NC010 is a 40% glass reinforced liquid crystal polymer resin having an excellent heat deflection temperature of 356°C.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³ISO 1183
Filler Content 40 %40 %Glass Reinforced
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 175 MPa
@Temperature 23.0 °C
25400 psi
@Temperature 73.4 °F
ISO 527
Elongation at Break 1.5 %
@Temperature 23.0 °C
1.5 %
@Temperature 73.4 °F
ISO 527
Tensile Modulus 18.0 GPa
@Temperature 23.0 °C
2610 ksi
@Temperature 73.4 °F
ISO 527
Flexural Strength 250 MPa
@Temperature 23.0 °C
36300 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 16.0 GPa
@Temperature 23.0 °C
2320 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  -2.00 µm/m-°C
@Temperature 160 - 320 °C
-1.11 µin/in-°F
@Temperature 320 - 608 °F
ISO 11359-1/-2
 3.00 µm/m-°C
@Temperature 55.0 - 160 °C
1.67 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
 -2.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 320 °C
-1.11 µin/in-°F
@Thickness 0.157 in,
Temperature 320 - 608 °F
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 23.0 °C
1.11 µin/in-°F
@Thickness 0.157 in,
Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 320 °C
1.11 µin/in-°F
@Thickness 0.157 in,
Temperature -40.0 - 608 °F
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.11 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 23.0 °C
1.11 µin/in-°F
@Thickness 0.0787 in,
Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 320 °C
1.11 µin/in-°F
@Thickness 0.0787 in,
Temperature -40.0 - 608 °F
ISO 11359-1/-2
 3.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
1.67 µin/in-°F
@Thickness 0.157 in,
Temperature 73.4 - 131 °F
ISO 11359-1/-2
 4.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
2.22 µin/in-°F
@Thickness 0.157 in,
Temperature 131 - 320 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow  48.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
26.7 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 55.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
30.6 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
 71.0 µm/m-°C
@Temperature 55.0 - 160 °C
39.4 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
 74.0 µm/m-°C
@Temperature -40.0 - 320 °C
41.1 µin/in-°F
@Temperature -40.0 - 608 °F
ISO 11359-1/-2
 88.0 µm/m-°C
@Temperature 160 - 320 °C
48.9 µin/in-°F
@Temperature 320 - 608 °F
ISO 11359-1/-2
 48.0 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 23.0 °C
26.7 µin/in-°F
@Thickness 0.157 in,
Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 55.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
30.6 µin/in-°F
@Thickness 0.157 in,
Temperature 73.4 - 131 °F
ISO 11359-1/-2
 71.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
39.4 µin/in-°F
@Thickness 0.157 in,
Temperature 131 - 320 °F
ISO 11359-1/-2
 75.0 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 320 °C
41.7 µin/in-°F
@Thickness 0.157 in,
Temperature -40.0 - 608 °F
ISO 11359-1/-2
 92.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 320 °C
51.1 µin/in-°F
@Thickness 0.157 in,
Temperature 320 - 608 °F
ISO 11359-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 356 °C673 °FISO 75-1/-2 1993/N2
UL RTI, Electrical 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
UL RTI, Mechanical with Impact 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
IEC 60695-11-10
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
UL94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 380 °C716 °FOptimum
 375 - 385 °C707 - 725 °F
Mold Temperature 80.0 °C176 °FOptimum
 40.0 - 150 °C104 - 302 °F
Drying Temperature 150 °C302 °F
Dry Time 3 hour3 hourDehumidified Dryer
Moisture Content <= 0.010 %<= 0.010 %
 
Descriptive Properties
AppearanceNatural Color
DuPont Product CategoryElectrical Resins
 Flame Retardant Resins
 Glass Reinforced Resins
FormPellets
Part Marking Code>LCP-GF40<ISO 11469
RegionAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-GF40ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zenite® 7140X BK010 LCP
Celanese VECTRA T.rex541 LCP, 40% Specialty
Celanese VECTRA® L140 40% Glass Reinforced Liquid Crystal Polymer (LCP)
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
Avient Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding

PDTA8782 / 31815

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.