MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 2161 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), Stainless Steel Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/ccASTM D 792
Additive Loading 10 %10 %Primary Additive
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0080 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 109 MPa15800 psiASTM D 638
Elongation at Break 5.0 - 9.0 %5.0 - 9.0 %ASTM D 638
Tensile Modulus 3.72 GPa540 ksiASTM D 638
Flexural Strength 152 MPa22000 psiASTM D 790
Flexural Modulus 4.00 GPa580 ksiASTM D 790
Izod Impact, Notched 0.427 J/cm
@Thickness 3.20 mm
0.800 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.87 J/cm
@Thickness 3.20 mm
11.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10 ohm-cm<= 10 ohm-cmASTM D 257
Surface Resistance <= 1e+05<= 1e+05ESD STM11.11
Surface Resistivity per Square <= 1.00e+6 ohm<= 1.00e+6 ohmASTM D 257
Static Decay <= 0.50 sec<= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 207 °C405 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 199 °C390 °FASTM D 648
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 354 - 399 °C670 - 750 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 14400 sec
300 °F
@Time 4.00 hour
Moisture Content 0.040 %0.040 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 300 TFE 20 SE Polycarbonate (PC), Unreinforced - PTFE Lubricated - Self Extinguishing - Bromine/Chlorine Free - UL94 V-0
RTP Company RTP 300 TFE 15 SE Polycarbonate (PC), Unreinforced - PTFE Lubricated - Self Extinguishing - Bromine/Chlorine Free - UL94 V-2
RTP Company RTP 1400 R-5100 Polyphenylsulfone (PPSU)

PQZUA3870 / 134878

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.