MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 85786A Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Grade for calandering; no yellowing under the action of UV light; good low-temperature flexibility; high rebound resilience; improved microbial resistance; Improved hydrolysis resistance; Application; Textile coating

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ISO 868
Tensile Strength, Ultimate 33.0 MPa4790 psi200 mm/min; DIN 53504
Tensile Stress at Strain  7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
200 mm/min; DIN 53504
 10.0 MPa
@Strain 300 %
1450 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 715 %715 %200 mm/min; DIN 53504
Tensile Modulus  0.0500 GPa
@Temperature 60.0 °C
7.25 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.0650 GPa
@Temperature 20.0 °C
9.43 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 0.260 GPa
@Temperature -20.0 °C
37.7 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
Rebound 64 %64 %Resilience; ISO 4662
Tear Strength 74.0 kN/m422 pli500 mm/min; ISO 34-1
Abrasion 3030mm³, Method A; ISO 4649
Compression Set  18 %
@Temperature 23.0 °C
18 %
@Temperature 73.4 °F
72 hr; ISO 815
 42 %
@Temperature 70.0 °C
42 %
@Temperature 158 °F
24 hr; ISO 815
 32 %
@Temperature 70.0 °C,
Time 86400 sec
32 %
@Temperature 158 °F,
Time 24.0 hour
200 mm/min; DIN 53504
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 190 °C338 - 374 °FInjection
 170 - 190 °C338 - 374 °FExtrusion
Mold Temperature 20.0 °C68.0 °FInjection
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 487 Thermoplastic Polyurethane
Covestro Desmopan® 9873DU Polyurethane
Covestro Desmopan® W DP 85085A Polyurethane
Covestro Desmopan® W DP89056D Polyurethane
Covestro Desmopan® W DP89043D Polyurethane

PB09827 / 92667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.