MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics TOPAS® Elastomer E-140 Cyclic Olefin Copolymer (COC)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be blended with other TOPAS grades, olefin resins and elastomers. For an elastomer, E-140 features high moisture barrier and has moderate clarity in thin sections or films. Secondary Tg of -6°C is relatively insignificant in terms of E-140 properties such as low temperature brittleness. Primary Tg is below -90°C, while the melting point is about 84°C.

Key applications and attributes:

  • High toughness film (as COC blend): Toughness, clarity, stiffness, low WVTR, reclaimability
  • Tubing: Purity, kink resistance
  • Bags: Purity, olefin compatibility
  • Over-molding: Adhesion to olefins, purity, soft feel
  • Food packaging: Not manufactured with BPA, phthalates, or halogens
  • Food contact: Broad regulatory approval

Note: 125µm film data includes 1% Ampacet 102765 1.5:1 BUR

Information provided by Polyplastics USA, which merged with TOPAS Advanced Polymers in 2018.

Key Words: Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oxygen Permeability 4240 cm3 mil/(m2 day atm)
@Temperature 23.0 °C
274 cm3 mil/(100 in2 day atm)
@Temperature 73.4 °F
50% RH; ISO 15105-2
Water Vapor Permeability 18.4 g mil/ (m2 day)
@Temperature 38.0 °C
1.19 g mil/ (100 in2 day)
@Temperature 100 °F
90% RH; ISO 15106-3
Density 0.940 g/cc0.0340 lb/in³ISO 1183
Thickness 127 microns5.00 mil
Melt Flow  2.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 11 g/10 min
@Load 2.16 kg,
Temperature 260 °C
11 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD  640 %
@Thickness 0.0500 mm
640 %
@Thickness 0.00197 in
ASTM D882
 800 %
@Thickness 0.125 mm
800 %
@Thickness 0.00492 in
ASTM D882
Film Elongation at Break, TD  620 %
@Thickness 0.0500 mm
620 %
@Thickness 0.00197 in
ASTM D882
 790 %
@Thickness 0.125 mm
790 %
@Thickness 0.00492 in
ASTM D882
Elmendorf Tear Strength MD  1103 g
@Load 3.20 kg,
Thickness 0.0500 mm
1103 g
@Load 7.06 lb,
Thickness 0.00197 in
ASTM D1922
 2718 g
@Load 0.00326 kg,
Thickness 3.17 mm
2718 g
@Load 0.00704 lb,
Thickness 0.125 in
ASTM D1922
Elmendorf Tear Strength TD  1221 g
@Load 3.20 kg,
Thickness 0.0500 mm
1221 g
@Load 7.06 lb,
Thickness 0.00197 in
ASTM D1922
 3171 g
@Load 0.00326 kg,
Thickness 0.125 mm
3171 g
@Load 0.00704 lb,
Thickness 0.00492 in
ASTM D1922
Film Tensile Strength at Break, MD  52.0 MPa
@Thickness 0.125 mm
7540 psi
@Thickness 0.00492 in
ASTM D882
 60.7 MPa
@Thickness 0.0500 mm
8800 psi
@Thickness 0.00197 in
ASTM D882
Film Tensile Strength at Break, TD  50.4 MPa
@Thickness 0.0500 mm
7310 psi
@Thickness 0.00197 in
ASTM D882
 50.6 MPa
@Thickness 0.125 mm
7340 psi
@Thickness 0.00492 in
ASTM D882
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.24
@Frequency 1e+9 Hz
2.24
@Frequency 1e+9 Hz
ASTM D2520B
Dielectric Strength 157 kV/mm4000 kV/inASTM D149-97a
Dissipation Factor 0.00026
@Frequency 1e+9 Hz
0.00026
@Frequency 1e+9 Hz
ASTM D2520B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 64.0 °C147 °FVST/A50; ISO 306
Brittleness Temperature <= 90.0 °C<= 194 °FISO 974
 
Optical PropertiesMetricEnglishComments
Haze  1.27 %
@Thickness 0.125 mm
1.27 %
@Thickness 0.00492 in
ASTM D1003
 1.5 %
@Thickness 0.0500 mm
1.5 %
@Thickness 0.00197 in
ASTM D1003
Gloss  94 %
@Thickness 0.0500 mm
94 %
@Thickness 0.00197 in
60°; ASTM D2457
 116 %
@Thickness 0.125 mm
116 %
@Thickness 0.00492 in
60°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 84.0 °C183 °FInternal Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013L-17 COC

POTOPAS16 / 142648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.