MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Isoplast® 2530 White ETPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Isoplast® 2530 White is an Engineered Thermoplastic Polyurethane (ETPU) designed for rigid polymer requirements due to their high tensile strength and impact resistance. They combine the toughness and dimensional stability of amorphous resins with the chemical resistance of crystalline PLUBR9s. It is ideal for applications needing an impact resistance-based polymer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.13 %
@Time 86400 sec
0.13 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5555ASTM D648
Hardness, Rockwell R 121121ASTM D648
Tensile Strength at Break 69.0 MPa10000 psiASTM D638
Tensile Strength, Yield 63.0 MPa9140 psiASTM D638
Elongation at Break 160 %160 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 1.90 GPa276 ksiASTM D638
Flexural Strength 90.0 MPa13100 psiASTM D790
Flexural Modulus 2.30 GPa334 ksiASTM D790
Izod Impact, Notched  0.590 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
1.11 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
 0.850 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.59 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy  75.0 J
@Temperature -29.0 °C
55.3 ft-lb
@Temperature -20.2 °F
ASTM D3763
 80.0 J
@Temperature 23.0 °C
59.0 ft-lb
@Temperature 73.4 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C178 °Funannealed; ASTM D648
 93.0 °C199 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °Funannealed; ASTM D648
 89.0 °C192 °Fannealed; ASTM D648
Vicat Softening Point 101 °C214 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Yellow Index 10 %10 %ASTM D1925
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 221 °C430 °FInjection
Front Barrel Temperature 226 °C439 °FInjection
Nozzle Temperature 232 °C450 °FInjection
Melt Temperature 221 - 243 °C430 - 469 °FInjection
Mold Temperature 66.0 - 82.0 °C151 - 180 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Isoplast® 2530 ETPU
Lubrizol LifeSciences Isoplast® 2560 ETPU
Lubrizol LifeSciences Carbothane® AC-4055D-B20 Aromatic TPU
Lubrizol LifeSciences Isoplast® 2531 ETPU
Lubrizol LifeSciences Isoplast® 2540 ETPU

PLUBR9021 / 203588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.