MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Lucent POM-900P Acetal Homopolymer, Easy Flow, Injection Grade
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Add "U" for UV Stabilized

Information provided by Lucent Polymers, Inc. Lucent was acquired by A. Schulman in 2015.

Key Words: POM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.020 cm/cm
@Thickness 3.17 mm
0.020 in/in
@Thickness 0.125 in
1/8" Section
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 68.97 MPa10000 psiASTM D638
Elongation at Break >= 20 %>= 20 %ASTM D638
Flexural Strength 100 MPa14500 psiASTM D790
Flexural Modulus 2.828 GPa410.1 ksiASTM D790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
1.30 ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 170 - 175 °C338 - 347 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 900P BK602 POM
Celanese Zytel® 70G13HS1L NC010 PA66-GF13
Asahi Kasei Tenac® SH710 Homopolymer Acetal Resin
A. Schulman Lucent POM-500 Acetal Homopolymer, General Purpose, Injection Grade
Delrin Delrin® 500P NC010 POM

PLUCE060 / 89979

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.