MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

7020-T6 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Similar in composition and properties to aluminum 7005.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 7020; AA7020; AFNOR AZ5G; UNS A97020; Al7020-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.78 g/cc0.100 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 350 MPa
@Thickness <=100 mm
>= 50800 psi
@Thickness <=3.94 in
Tensile Strength, Yield >= 280 MPa
@Thickness <=100 mm
>= 40600 psi
@Thickness <=3.94 in
0.2% offset
Elongation at Break >= 10 %
@Thickness <=100 mm
>= 10 %
@Thickness <=3.94 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000493 ohm-cm0.00000493 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.1 µm/m-°C
@Temperature 20.0 - 100 °C
12.8 µin/in-°F
@Temperature 68.0 - 212 °F
 24.0 µm/m-°C
@Temperature 20.0 - 200 °C
13.3 µin/in-°F
@Temperature 68.0 - 392 °F
 25.0 µm/m-°C
@Temperature 20.0 - 300 °C
13.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.875 J/g-°C
@Temperature 0.000 - 100 °C
0.209 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 137 W/m-K951 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 470 °C878 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.2 - 94.7 %91.2 - 94.7 %As remainder
Chromium, Cr 0.10 - 0.35 %0.10 - 0.35 %
Copper, Cu <= 0.20 %<= 0.20 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 1.0 - 1.4 %1.0 - 1.4 %
Manganese, Mn 0.05 - 0.50 %0.05 - 0.50 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.35 %<= 0.35 %
Zinc, Zn 4.0 - 5.0 %4.0 - 5.0 %
Zirconium, Zr 0.08 - 0.20 %0.08 - 0.20 %
Zr+Ti 0.08 - 0.25 %0.08 - 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
7020-T652 Aluminum
Aluminum 7021-T62
Aluminum 7075-T6; 7075-T651
Overview of materials for 7000 Series Aluminum Alloy
Aluminum 7034-T6

MA7020n / 9547

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.