MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE; Polypropylene (PP)

Material Notes: Product Description: Exxelor Po 1015 polymer resin is a maleic anhydride fuctionalized polypropylene copolymer, produced by reactive extrusion. It has been primarily designed to add polarity to polypropylene matrices and in particular improved polypropylene reactivity and amio-silane treated glass reinforcements. This grade is designed to:
  • Function as a coupling agent between reinforcing materials such as glass fibers and inorganic fillers, and polypropylene.
  • Achieve compatibility in polypropylene/polyamide alloys.
  • Achieve compatibility between polyolefins and more polar polymers that are capable of interaction with maleic anhydride for alloying recycling or co-extrusion purpose.
  • Improve polypropylene-to-metal adhesion properties.

Key Features: Performance enhancements in glass-filled polypropylene:

  • Outstanding unnotched Izod and Charpy impact performance
  • Excellent notched Izod and Charpy impact resistance
  • Improved tensile and flexural strength
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³DIN 53479
Melt Flow  22 g/10 min
@Load 1.20 kg,
Temperature 190 °C
22 g/10 min
@Load 2.65 lb,
Temperature 374 °F
ASTM D1238
 150 g/10 min
@Load 2.16 kg,
Temperature 190 °C
150 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Collected Volatile Condensable Material <= 0.20 %<= 0.20 %AM-S 350.03
 
Thermal PropertiesMetricEnglishComments
Melting Point 138 °C280 °FPeak; DSC
 
Optical PropertiesMetricEnglishComments
Yellow Index <= 20 %<= 20 %ASTM E313-96
 
Descriptive Properties
Maleic anhydride graft levelmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene
ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin
ExxonMobil EXXELOR™ VA 1840 Maleic anhydride functionalized elastomeric ethylene copolymer
ExxonMobil EXXELOR™ VA 1801 Maleic anhydride functionalized elastomeric ethylene copolymer
ExxonMobil EXXELOR™ VA 1803 Maleic anhydride functionalized elastomeric ethylene copolymer

PEXB512 / 37817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.