MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings
Categories: Ceramic; Glass; Glass Ceramic; Machinable Ceramic

Material Notes: Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardness) typical of ceramics. It is made by mixing the components in powder form and heated under pressure. The glass particles melt and cover the mica flakes to form a hard, compact mass. It does not burn, is not hygroscopic, has high resistivity, is suitable for vacuum use, and has generally good chemical resistance - it is attacked by acetic, hydrochloric and nitric acid but resists sulfuric and phosphoric acids, ammonia, caustic soda, organic solvents, and saline solutions.

Applications include electric traction (railways, subways), busbar mountings, terminals, power cable mountings, switchbox mountings, and insulation of heating elements.

Information provided by Saint-Gobain Quartz PLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.30 g/cc0.155 lb/in³
Water Absorption 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8080
Tensile Strength, Ultimate 20.0 MPa2900 psi
Elongation at Break 0.50 %0.50 %
Flexural Strength 80.0 MPa11600 psiBending Strength
Compressive Strength 260 MPa37700 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.60e+13 ohm-cm1.60e+13 ohm-cm
Surface Resistance 3.00e+14 ohm3.00e+14 ohm
Dielectric Constant 11
@Frequency 1000 Hz
11
@Frequency 1000 Hz
Dielectric Strength 11.0 kV/mm279 kV/in
Dissipation Factor 0.017 - 0.040
@Frequency 1000 Hz
0.017 - 0.040
@Frequency 1000 Hz
Arc Resistance 320 sec320 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 °C
6.11 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.700 W/m-K
@Temperature 250 °C
4.86 BTU-in/hr-ft²-°F
@Temperature 482 °F
Maximum Service Temperature, Air 350 °C662 °F
Softening Point 420 °C788 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Compression Moldings
Aclo Accutech Polypropylene Homopolymer HP0334M10L Mica Reinforced
Crystex Composites Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite
Imerys 160D Ground Mica
LKAB Minerals Muscovite Mica

CSTGQZ26 / 2298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.