MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Pellethane® 5863-91A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Aromatic Polyether-based Thermoplastic Polyurethane (TPU)

Features: High melt flow and good temperature resistance

Extrusion Grade

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240
Tensile Strength, Ultimate 38.3 MPa5550 psiASTM D412
Elongation at Break 525 %525 %ASTM D412
100% Modulus 9.00 MPa
@Strain 100 %
1310 psi
@Strain 100 %
ASTM D412
300% Modulus 17.2 MPa
@Strain 300 %
2490 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0377 GPa5.47 ksiASTM D790
Tear Strength 17.9 kN/m102 pliTrouser; ASTM D470
Graves Tear Strength 59.6 kN/m340 plidie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 41
@Load 1.00 kg
41
@Load 2.20 lb
H-18; ASTM D3389
Compression Set  25 %
@Temperature 23.0 °C,
Time 79200 sec
25 %
@Temperature 73.4 °F,
Time 22.0 hour
 60 %
@Temperature 70.0 °C,
Time 79200 sec
60 %
@Temperature 158 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -44.0 °C-47.2 °F
 
Processing PropertiesMetricEnglishComments
Zone 1 177 °C351 °F
Zone 2 182 °C360 °F
Zone 3 191 °C376 °F
Zone 4 196 °C385 °F
Adapter Temperature 199 °C390 °F5
Die Temperature 194 °C381 °F2
 196 °C385 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecoflex® EG-93A-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2095A-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2095A-B20 TPU – 20% Barium Sulfate
Dow Silastic® Q7-4780 BIOMEDICAL GRADE ETR ELASTOMER, KIT
Lubrizol LifeSciences Pellethane® 2363-90AE TPU

PLUBR9039 / 203606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.