MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos ABS Centrex® 401 AES Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; AES Polymer; AES, Extruded

Material Notes: Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with <10% orientation.

Information provided by Bayer Corporation, Plastics Division

LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS. This product is no longer listed as a standard NAFTA product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Melt Flow 5.6 g/10 min
@Load 10.0 kg,
Temperature 230 °C
5.6 g/10 min
@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9191ASTM D785
Tensile Strength, Ultimate 24.0 MPa3480 psiASTM D638
Tensile Strength, Yield 29.0 MPa4210 psiASTM D638
Tensile Modulus 1.70 GPa247 ksiASTM D638
Flexural Yield Strength 42.1 MPa6110 psiASTM D790
Flexural Modulus 1.50 GPa218 ksiASTM D790
Izod Impact, Notched 0.910 J/cm
@Temperature -40.0 °C
1.70 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 5.90 J/cm
@Thickness 3.17 mm
11.1 ft-lb/in
@Thickness 0.125 in
ASTM D256
Impact Test 35.0 J
@Thickness 3.20 mm
25.8 ft-lb
@Thickness 0.126 in
Instrumented Impact, Total Energy; 3.2 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec
@Thickness 3.35 mm
60 - 120 sec
@Thickness 0.132 in
UL Rating PLC 6 (60-120 sec)
Comparative Tracking Index >= 600 V
@Thickness 3.35 mm
>= 600 V
@Thickness 0.132 in
UL Rating PLC 0 (>600 V)
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 3.35 mm
15 - 30 sec
@Thickness 0.132 in
UL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.43 mm
>= 120 arcs
@Thickness 0.0563 in
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
@Thickness 1.43 mm
0.394 - 1.00 in/min
@Thickness 0.0563 in
UL Rating PLC 1 (10-25.4 mm/min.)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 79.0 µm/m-°C
@Temperature 20.0 °C
43.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
@Thickness 3.17 mm
174 °F
@Thickness 0.125 in
Unannealed; ASTM D648
UL RTI, Electrical 50.0 °C
@Thickness 1.60 mm
122 °F
@Thickness 0.0630 in
UL746B
UL RTI, Mechanical with Impact 50.0 °C
@Thickness 1.60 mm
122 °F
@Thickness 0.0630 in
UL746B
UL RTI, Mechanical without Impact 50.0 °C
@Thickness 1.60 mm
122 °F
@Thickness 0.0630 in
UL746B
Flammability, UL94  HB
@Thickness 1.43 mm
HB
@Thickness 0.0563 in
 HB
@Thickness 1.43 mm
HB
@Thickness 0.0563 in
 
Optical PropertiesMetricEnglishComments
Gloss 45 %45 %60°; Formed; ASTM D523
 75 %75 %60°; Sheet; ASTM D523
Transmission, Visible 0.00 %0.00 %Opaque only
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 243 °C399 - 469 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond TR 5000
Ineos ABS NOVODUR® KU 2-5296 ABS, Extrusion Grade
Mitsubishi Xantar® 24 R Polycarbonate
Trinseo Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Ineos ABS Lustran® 130

PB1C10 / 26410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.