MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

FKuR Kunststoff Terralene® PP 2509 Biobased Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Terralene® PP 2509 is a biobased material optimized for injection molding applications. The processing and application characteristics of this material can be entirely compared to those of PP based on fossil materials. Terralene® PP 2509 offers a high flowability which is necessary e. g. for the production of complex components and products with long flow paths. This grade is based on about 35 % of renewable resources. This bio-based carbon content can be easily verified with the help of the C-14 method according to ASTM D 6866. Polypropylene copolymer blend with biobased high density polyethylene. The biobased carbon content (BCC) is 33 %. Suitable for injection molding applications such as bins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.916 g/cc0.0331 lb/in³ISO 1183
Melt Flow 33 - 37 g/10 min
@Load 2.16 kg,
Temperature 190 °C
33 - 37 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 9.00 MPa1310 psiISO 527
Tensile Strength, Ultimate 20.5 MPa2970 psiISO 527
Tensile Strength, Yield 21.0 MPa3050 psiISO 527
Elongation at Break 135 %135 %ISO 527
Modulus of Elasticity 0.910 GPa132 ksiISO 527
Tensile Modulus 0.910 GPa132 ksiISO 527
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1/1 eU
Charpy Impact, Notched 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
partial break; ISO 179-1/1 eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FISO 3146-C
Vicat Softening Point 117 °C243 °FISO 306
 
Descriptive Properties
Bio-based carbon content (%)33ASTM D 6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cyclewood Solutions Xylomer™ XM2-FPC Sustainable Injection Molding Resin
Cyclewood Solutions Xylomer™ XM2-CUA Sustainable Injection Molding Resin
Cyclewood Solutions Xylomer™ XM2-JNA Sustainable Injection Molding Resin
Mitsubishi Chemical Advanced Materials Proteus™ LSG HS PP-H Heat Stabilized Polypropylene
Miracll G365 Bio-based Polyester TPU

PFKUR924 / 192732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.