MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ampco Metal AMPCO® 21 Aluminum Bronze, Rectangular
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: The increase in the Al and Fe content results in a material in which the hard gamma 2 phase (about 400 HB) is present. By proper metallurgical control this hard constituent is uniformly distributed giving this alloy its ability to resist wear.

Applications: AMPCO 21 is used for guide port bushings and wear strips replacing hardened steel and for some cams when no impact is involved. However, the largest single use is as die rings, inserts, forming rolls etc. in forming, bending or drawing operations, especially when stainless steel is the material being processed. This material is also widely used as work support blades for the centreless grinding of steel rods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.20 g/cc0.260 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 286286HB 30
Hardness, Rockwell C 2929
Tensile Strength, Ultimate 758 MPa110000 psi
Tensile Strength, Yield 420 MPa
@Strain 0.5 %
60900 psi
@Strain 0.5 %
Elongation at Break 1.0 %1.0 %
Reduction of Area 0.50 %0.50 %
Modulus of Elasticity 110 GPa16000 ksi
Compressive Yield Strength 343 MPa49700 psi0.1% Perm. Set
Compressive Strength 1108 MPa160700 psi
Shear Strength 413 MPa59900 psi
Izod Impact 2.70 J1.99 ft-lb
Charpy Impact 2.70 J1.99 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000167 ohm-cm0.0000167 ohm-cm10% I.A.C.S.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 °C
9.00 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 46.0 W/m-K319 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 13.1 %13.1 %
Copper, Cu 80 - 80.5 %80 - 80.5 %As Balance
Iron, Fe 4.4 %4.4 %
Manganese, Mn 2.0 %2.0 %
Other, total <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum bronze 5%, UNS C60800
AISI Type H13 Hot Work Tool Steel
Ampco Metal AMPCO® 8 Aluminum Bronze, Extruded and Drawn Rods, 12.7 - 25.4 mm.
Ampco Metal AMPCO® 22 Aluminum Bronze, Extruded Bar
Ampco Metal AMPCO® 21 Aluminum Bronze, Round, ≤ 50.8 mm.

NAMPCO17 / 14971

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.