MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Kennametal Stellite Stellite® 98M2 cast
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite, Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.45 g/cc0.305 lb/in³P/M (98%)
 8.63 g/cc0.312 lb/in³Theoretical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 6060Hot hardness.
Tensile Strength, Ultimate 518 MPa75100 psi
Elongation at Break <= 1.0 %<= 1.0 %in 25.4 mm
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability <= 1.2
@Temperature 22.0 °C
<= 1.2
@Temperature 71.6 °F
116 Oersted
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.8 µm/m-°C
@Temperature 20.0 - 100 °C
6.00 µin/in-°F
@Temperature 68.0 - 212 °F
 11.1 µm/m-°C
@Temperature 20.0 - 200 °C
6.17 µin/in-°F
@Temperature 68.0 - 392 °F
 11.5 µm/m-°C
@Temperature 20.0 - 300 °C
6.39 µin/in-°F
@Temperature 68.0 - 572 °F
 11.7 µm/m-°C
@Temperature 20.0 - 400 °C
6.50 µin/in-°F
@Temperature 68.0 - 752 °F
 12.1 µm/m-°C
@Temperature 20.0 - 500 °C
6.72 µin/in-°F
@Temperature 68.0 - 932 °F
 12.7 µm/m-°C
@Temperature 20.0 - 600 °C
7.06 µin/in-°F
@Temperature 68.0 - 1110 °F
 13.0 µm/m-°C
@Temperature 20.0 - 700 °C
7.22 µin/in-°F
@Temperature 68.0 - 1290 °F
 13.4 µm/m-°C
@Temperature 20.0 - 800 °C
7.44 µin/in-°F
@Temperature 68.0 - 1470 °F
 13.7 µm/m-°C
@Temperature 20.0 - 900 °C
7.61 µin/in-°F
@Temperature 68.0 - 1650 °F
 14.1 µm/m-°C
@Temperature 20.0 - 1000 °C
7.83 µin/in-°F
@Temperature 68.0 - 1830 °F
Melting Point 1224 - 1275 °C2235 - 2327 °F
Solidus 1224 °C2235 °F
Liquidus 1275 °C2327 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 1.0 %1.0 %
Carbon, C 2.0 %2.0 %
Chromium, Cr 30 %30 %
Cobalt, Co 31 %31 %As remainder
Iron, Fe <= 5.0 %<= 5.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo <= 0.80 %<= 0.80 %
Nickel, Ni 3.5 %3.5 %
Other <= 2.0 %<= 2.0 %
Silicon, Si <= 1.0 %<= 1.0 %
Tungsten, W 18.5 %18.5 %
Vanadium, V 4.2 %4.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy
Kennametal Stellite Stellite® 3 PM cast
Kennametal Stellite Stellite® 6 PM cast
Kennametal Stellite Stellite® 190 PM with P/M Processing
Kennametal Stellite Stellite® 21

NS98MB / 18890

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.