MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 1118 Steel, cold drawn, high temperature, stress relieved, round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Applications include medium duty shafts, studs, pins, distributor cams, cam shafts, and universal joints.

Key Words: NS G11180, ASTM A29, ASTM A107, ASTM A108, FED QQ-S-637 (C1118), SAE J403, SAE J412, SAE J414
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steel.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  111
@Diameter 50.8 - 76.2 mm
111
@Diameter 2.00 - 3.00 in
 121
@Diameter 31.8 - 50.8 mm
121
@Diameter 1.25 - 2.00 in
 131
@Diameter 22.2 - 31.8 mm
131
@Diameter 0.875 - 1.25 in
 143
@Diameter 15.9 - 22.2 mm
143
@Diameter 0.625 - 0.875 in
Hardness, Knoop  129
@Diameter 50.8 - 76.2 mm
129
@Diameter 2.00 - 3.00 in
Converted from Brinell
 140
@Diameter 31.8 - 50.8 mm
140
@Diameter 1.25 - 2.00 in
Converted from Brinell
 150
@Diameter 22.2 - 31.8 mm
150
@Diameter 0.875 - 1.25 in
Converted from Brinell
 163
@Diameter 15.9 - 22.2 mm
163
@Diameter 0.625 - 0.875 in
Converted from Brinell
Hardness, Rockwell B  64
@Diameter 50.8 - 76.2 mm
64
@Diameter 2.00 - 3.00 in
Converted from Brinell
 68
@Diameter 31.8 - 50.8 mm
68
@Diameter 1.25 - 2.00 in
Converted from Brinell
 73
@Diameter 22.2 - 31.8 mm
73
@Diameter 0.875 - 1.25 in
Converted from Brinell
 78
@Diameter 15.9 - 22.2 mm
78
@Diameter 0.625 - 0.875 in
Converted from Brinell
Hardness, Vickers  115
@Diameter 50.8 - 76.2 mm
115
@Diameter 2.00 - 3.00 in
Converted from Brinell
 126
@Diameter 31.8 - 50.8 mm
126
@Diameter 1.25 - 2.00 in
Converted from Brinell
 136
@Diameter 22.2 - 31.8 mm
136
@Diameter 0.875 - 1.25 in
Converted from Brinell
 149
@Diameter 15.9 - 22.2 mm
149
@Diameter 0.625 - 0.875 in
Converted from Brinell
Tensile Strength, Ultimate  380 MPa
@Diameter 50.8 - 76.2 mm
55100 psi
@Diameter 2.00 - 3.00 in
 415 MPa
@Diameter 31.8 - 50.8 mm
60200 psi
@Diameter 1.25 - 2.00 in
 450 MPa
@Diameter 22.2 - 31.8 mm
65300 psi
@Diameter 0.875 - 1.25 in
 485 MPa
@Diameter 15.9 - 22.2 mm
70300 psi
@Diameter 0.625 - 0.875 in
Tensile Strength, Yield  310 MPa
@Diameter 50.8 - 76.2 mm
45000 psi
@Diameter 2.00 - 3.00 in
 345 MPa
@Diameter 15.9 - 22.2 mm
50000 psi
@Diameter 0.625 - 0.875 in
 345 MPa
@Diameter 22.2 - 31.8 mm
50000 psi
@Diameter 0.875 - 1.25 in
 345 MPa
@Diameter 31.8 - 50.8 mm
50000 psi
@Diameter 1.25 - 2.00 in
Elongation at Break  15 %
@Diameter 31.8 - 50.8 mm
15 %
@Diameter 1.25 - 2.00 in
in 50 mm
 15 %
@Diameter 50.8 - 76.2 mm
15 %
@Diameter 2.00 - 3.00 in
in 50 mm
 16 %
@Diameter 22.2 - 31.8 mm
16 %
@Diameter 0.875 - 1.25 in
in 50 mm
 18 %
@Diameter 15.9 - 22.2 mm
18 %
@Diameter 0.625 - 0.875 in
in 50 mm
Reduction of Area  40 %
@Diameter 31.8 - 50.8 mm
40 %
@Diameter 1.25 - 2.00 in
 40 %
@Diameter 50.8 - 76.2 mm
40 %
@Diameter 2.00 - 3.00 in
 45 %
@Diameter 15.9 - 22.2 mm
45 %
@Diameter 0.625 - 0.875 in
 45 %
@Diameter 22.2 - 31.8 mm
45 %
@Diameter 0.875 - 1.25 in
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel.
Izod Impact 103 J76.0 ft-lbnormalized at 925°C (1700°F)
 107 J78.9 ft-lbannealed at 790°C (1450°F)
 108 J79.7 ft-lbas rolled
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000174 ohm-cm0.0000174 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 °C
6.39 µin/in-°F
@Temperature 68.0 °F
Typical steel
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
6.78 µin/in-°F
@Temperature 32.0 - 572 °F
Typical for steel
 13.9 µm/m-°C
@Temperature 0.000 - 500 °C
7.72 µin/in-°F
@Temperature 32.0 - 932 °F
Typical for steel
Specific Heat Capacity 0.472 J/g-°C0.113 BTU/lb-°FTypical steel
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.14 - 0.20 %0.14 - 0.20 %
Iron, Fe 98.03 - 98.48 %98.03 - 98.48 %As remainder
Manganese, Mn 1.3 - 1.6 %1.3 - 1.6 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S 0.080 - 0.13 %0.080 - 0.13 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1117 Steel, cold drawn, high temperature, stress relieved, round
AISI 1118 Steel, cold drawn, low temperature, stress relieved, round
AISI 1118 Steel, as cold drawn, round
AISI 1117 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1117 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

M1118L / 7165

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.