System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Hippe PF CC 203 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Categories:
Polymer
;
Thermoset
;
Phenolic
Material Notes:
Used in mechanical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts. Better mechanical properties and poorer electrical properties than type PF CC 204.
Information provided by Hippe.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.30
-
1.40
g/cc
1.30
-
1.40
g/cc
IEC 1212-2 8.1
Mechanical Properties
Metric
English
Comments
Tensile Strength
>=
85.0
MPa
>=
12300
psi
IEC 1212-2 5.7
Flexural Strength
>=
110
MPa
>=
16000
psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus
>=
7.00
GPa
>=
1020
ksi
IEC 1212-2 5.2
Shear Strength
>=
25.0
MPa
>=
3630
psi
Parallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO)
>=
5.90
kJ/m²
>=
2.81
ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched
>=
0.700
J/cm²
>=
3.33
ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Electrical Properties
Metric
English
Comments
Insulation Resistance
>=
1.00e+6
ohm
>=
1.00e+6
ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Breakdown
>=
1000
V
@Temperature 90.0 °C
>=
1000
V
@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Comparative Tracking Index
>=
100
V
>=
100
V
IEC 1212-2 6.4
Descriptive Properties
Thermal Endurance
120 T.I.
IEC 1212-2 7.1
Water Absorption
< 319 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Hippe PF CC 202 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Hexcel® HexWeb® HRH-78 - 3/8 - 1.5 Commercial Grade Nomex Honeycomb/Phenolic Resin
Hippe PF CC 31 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod
Bakelite® PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
PHIPPE914 / 121918
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.