MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cossa Polimeri ESTAPROP H 0360 T8 Polypropylene, 30% Mineral Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade; Polypropylene, Mineral Reinforced

Material Notes: PP homopolymer 30% mineral filler

Extrusion grade

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D 792
Linear Mold Shrinkage 0.012 - 0.014 cm/cm0.012 - 0.014 in/inASTM D 955
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 23.0 MPa3340 psiASTM D 638
Tensile Strength, Yield 27.0 MPa3920 psiASTM D 638
Elongation at Break 30 %30 %ASTM D 638
Tensile Modulus 3.60 GPa522 ksiASTM D 638
Flexural Modulus 3.20 GPa464 ksiASTM D 790
Izod Impact, Notched  0.150 J/cm
@Temperature -20.0 °C
0.281 ft-lb/in
@Temperature -4.00 °F
ASTM D 638
 0.250 J/cm
@Temperature 0.000 °C
0.468 ft-lb/in
@Temperature 32.0 °F
ASTM D 638
 0.350 J/cm
@Temperature 23.0 °C
0.656 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °F120°C/hr; ASTM D 648
Vicat Softening Point 95.0 °C
@Load 5.00 kg
203 °F
@Load 11.0 lb
50°C/hr; ASTM D 1525
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cossa Polimeri ESTAPROP H 2550 CBS/E Polypropylene, 25% Mineral Filled
Inno-Comp INNOPOL® CS 1-5830 30% Glass-Fiber-Filled Polypropylene Homopolymer
Plastcom SLOVAMID 66 W 30 Polyamide 66, 30% Mineral Filled
Polykemi AB POLYfill PPC T2020 Polypropylene Copolymer, Mineral Reinforced
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled

PCOSSA805 / 156395

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.