MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Addiplast Addinyl C2 R Nylon 66/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: High impact resistance

Information provided by Addiplast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272Conditioned; ISO 868
 7878ISO 868
Tensile Strength, Yield 35.0 MPa5080 psiConditioned; ISO R 527
 55.0 MPa7980 psiISO R 527
Elongation at Yield 50 %50 %ISO R 527
 >= 50 %>= 50 %Conditioned; ISO R 527
Modulus of Elasticity 0.600 GPa87.0 ksiConditioned; ISO 178
 1.90 GPa276 ksiISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180/1A
 20.0 kJ/m²9.52 ft-lb/in²Conditioned; ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/IeU
 NBNBConditioned; ISO 179/IeU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/IeA
 NBNBConditioned; ISO 179/IeA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmConditioned; CEI 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmCEI 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmConditioned; CEI 60093
 1.00e+15 ohm1.00e+15 ohmCEI 60093
Comparative Tracking Index 600 V600 VCEI 60112/Solution A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM E831
Melting Point 243 °C469 °FISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75-2/AF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ AB700 UF Polyamide 66/6 Copolymer (Nylon 66/6)
Celanese Nilit FRIANYL C73 HS28 Nylon 6.6/6 for injection molding
EMS-Grivory Grilon® TSS PA666
Quadrant Symalit® 1000 PFA unfilled, lining industries (ISO Data)
Celanese Nilit FRIANYL C73 T Nylon 6.6/6 for injection molding

PFADD894 / 156108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.