MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cyclohexanone, C6H10O
Categories: Fluid; Solvent

Key Words: C6H10O
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc
@Temperature 20.0 °C
0.0344 lb/in³
@Temperature 68.0 °F
Viscosity 2.217 cP
@Temperature 20.0 °C
2.217 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 95.145 g/mol95.145 g/mol
Surface Tension 35.19 dynes/cm
@Temperature 20.0 °C
35.19 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 38.6 bar29000 torr
Critical Temperature 356 °C673 °F
Critical Density 0.305 g/cc0.0110 lb/in³
Critical Molar Volume 312 cm³/mol19.0 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 16.1
@Temperature 20.0 °C
16.1
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 417.8 J/g179.7 BTU/lb
Specific Heat Capacity 1.151 J/g-°C
@Temperature 25.0 °C
0.2751 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1403 W/m-K
@Temperature 20.0 °C
0.9737 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -31.2 °C-24.2 °F
Boiling Point 155.7 °C312.3 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45
@Wavelength 589.3 nm
1.45
@Wavelength 589.3 nm
nD
 
Descriptive Properties
CAS registry number (CARN)108-94-1
Chemical FormulaC6H10O
Critical Compressibility (Zc)0.23
Dipole moment (p/C.m)1.034E-27
Henry's Law Constant (atm m3/mol)5.11E-05
Molar Heat Capacity (298K)109.501 J/mol-K
Molar Heat Capacity of Vapor a Parameter-37.7815
Molar Heat Capacity of Vapor b Parameter0.5535
Molar Heat Capacity of Vapor c Parameter-0.0001952
Molar Heat Capacity of Vapor d Parameter-1.533E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number2256

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ MX731 Medical Grade Copolyester
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating
LyondellBasell Purell ACP 6541A High Density Polyethylene (HDPE), Injection Molded
INEOS Styrolution Terlux® HD 2802 MABS
Wacker Elastosil® R 401/60 Silicone Rubber

VORGS085 / 99469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.