MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Rilsan® Clear G850 Rnew® PA
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
 1.01 g/cc0.0365 lb/in³Cond.; ISO 1183
Water Absorption 4.0 %4.0 %Dry; Sim. to ISO 62
Moisture Absorption 1.70 %1.70 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inDry; ISO 294-4, 2577
 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 78
@Time 15.0 sec
78
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength, Yield 61.0 MPa8850 psiCond.; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 8.0 %8.0 %Cond.; ISO 527-1/-2
Tensile Modulus 1.67 GPa242 ksiCond.; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 0.750 J/cm²
@Temperature 23.0 °C
3.57 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FDry; ISO 75-1/-2
Glass Transition Temp, Tg 150 °C302 °F10°C/min; Dry; ISO 11357-1/-2
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Yellow Card Available; Dry; IEC 60695-11-10
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 92 %92 %Luminous; ISO 13468-1, -2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
 
Descriptive Properties
%Bio-Based45ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Moisture SensitiveYes
Processing MethodsInjection Molding
TransparentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsan® Clear G300 HI PA
Arkema Rilsan® BUM 30 O PA11-GB30
Arkema Rilsan® BSR 30 PA11-CF30
Arkema Rilsan® Clear G170 Polyamide
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer

PARKF916 / 193651

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.