MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stiffness and strength; outstanding mechanical and electrical properties.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Water Absorption 4.4 - 5.0 %4.4 - 5.0 %ISO 62
Moisture Absorption at Equilibrium 1.0 - 1.4 %1.0 - 1.4 %(23°C/50% R.H.); ISO 62
Viscosity Number 140 cm³/g1.40 dl/gISO 307
Linear Mold Shrinkage 0.0045 cm/cm0.0045 in/in
Melt Flow 43.5 g/10 min
@Load 5.00 kg,
Temperature 275 °C
43.5 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 120 MPa17400 psi50mm/min; ISO 527
Elongation at Yield 4.0 %4.0 %50mm/min; ISO 527
Modulus of Elasticity 8.50 GPa1230 ksiISO 527
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179/1eA
Tensile Creep Modulus, 1000 hours 4250 MPa616000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.20
@Frequency 1e+6 Hz
0.20
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.40 J/g-°C0.335 BTU/lb-°F
Thermal Conductivity 0.340 W/m-K2.36 BTU-in/hr-ft²-°FDIN 52612
Melting Point 260 °C500 °FTest Solution A; DIN 53765
Maximum Service Temperature, Air 140 °C284 °Ffor 50% loss of tensile strength after 20,000 hr
 157 °C315 °Ffor 50% loss of tensile strength after 5,000 hr
 220 °C428 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection-molding/Extrusion
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection-molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicFlame retarding agent
 Heat stabilized or stable to heat
 Release agent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Envalior Durethan® ECO BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
Domo TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Domo TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry

PBASF9272 / 85036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.