MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow INFUSE™ 9817 Olefin Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Material Notes: INFUSE™ 9817 Olefin Block Copolymer is a high performance olefin block copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. INFUSE 9817 has a higher set up temperature, which allows for faster injection molding cycle times. In addition, its high crystallization temperature and lower density drive lower production costs by reducing cycle time and reducing part weight.

Main Characteristics:

  • High upper service temperature performance
  • Highly flexible with good elastic recovery
  • Fast set up times for processability
  • General purpose elastomer
  • Excellent for compounds and blends
  • Talc dusted
Complies with
  • EU, No 10/2011
  • US FDA FCN 424
Consult the regulations for complete details.

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.877 g/cc0.0317 lb/in³ASTM D792
Melt Index of Compound 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7171Compression Molded; ASTM D2240
Tensile Strength at Break 7.00 MPa1020 psiCompression Molded; ASTM D638
 7.00 MPa1020 psiElastomer; ASTM D412
Elongation at Break 1500 %1500 %Compression Molded; ASTM D638
 1700 %1700 %Elastomer; ASTM D412
Tensile Modulus 0.00231 GPa0.335 ksi100% Secant (Compression Molded); ASTM D638
Tear Strength 31.0 kN/m177 pliASTM D624
Compression Set  15 %
@Temperature 21.0 °C
15 %
@Temperature 69.8 °F
ASTM D395
 58 %
@Temperature 70.0 °C
58 %
@Temperature 158 °F
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 120 °C248 °FDSC
 
Descriptive Properties
TMA@ 1.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
Noble Polymers Regis™ 315107 Thermoplastic Olefin (TPO)
RTP Company Permaprene™ 2800 B-65A Thermoplastic Polyolefin Elastomer (TEO)
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer

PDOW2032 / 183679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.