MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA214000 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Applications
PETROTHENE NA 214-000 is a low density polyethylene resin specifically designed for high speed, light weight, extrusion coating applications. This resin can be drawn down to a coating weight of three pounds per ream at line speeds exceeding 1,500 fpm with minimum neck-in and no edge weave. NA 214-000 can be used for applications including sugar pouches, industrial and multi-wall bags, treated and primed films and laminations.

Regulatory Status
NA 214-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply.

Processing Techniques
A melt temperature of 590°-620°F is recommended for use in processing NA 214-000 in light-weight coating applications. Electrostatic, flame or chemical priming should be used to ensure good adhesion. The maximum melt temperature that is recommended for NA 214-000 is 625°F.

Physical Properties
These are typical values and not to be construed as specific product limits.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454ASTM D2240
Tensile Strength at Break 10.9 MPa1580 psiType IV specimen; ASTM D638
Elongation at Break 580 %580 %Type IV specimen; ASTM D638
Flexural Stiffness 145 MPa21000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 86.0 °C187 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem BC818 Extrusion Coating Low Density Polyethylene
Braskem BI 818 LDPE Injection Molding Polyethylene
Braskem H502-25RG Extrusion Polypropylene
Dow 4010 Low Density Polyethylene (LDPE)
Lotte Chemical Titan TITANLENE® LDC800YY Low density polyethylene resin

PEQU0528 / 36996

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.