MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter No. 610® High Carbon, High Chrome Tool Steel (Air-Wear) (AISI D2)
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel; Air-Hardening Steel

Material Notes: No. 610 tool steel is an air hardening, high-carbon, high-chromium tool steel having extremely high wear resisting properties. It is very deep hardening, and will be practically free from size change after proper treatment. The high percentage of chromium gives it mild corrosion resisting properties in the hardened condition. It is available as a DeCarb-Free product. DCF bars have been cold-finished in the mill therefore eliminating the need for bar bark removal.

Applications: Blanking dies, Forming dies, Coining Dies, Slitting cutters, Heading tools, Long punches, Forming rolls, Edging Rolls, Master tools, Beading tools, Intricate punches, Extrusion dies, Drawing dies

Information provided by Carpenter Technology Corporation.

No. 610® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS T30402
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.83 g/cc7.83 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 44 - 4544 - 45Tempered at 1200°F
 62 - 6362 - 63As hardened
Abrasion 37.637.6loss in mm3, As-Hardened; ASTM G65
 85.985.9loss in mm3, Tempered at 1200°F; ASTM G65
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.5 µm/m-°C
@Temperature 20.0 - 100 °C
5.83 µin/in-°F
@Temperature 68.0 - 212 °F
 12.2 µm/m-°C
@Temperature 20.0 - 400 °C
6.78 µin/in-°F
@Temperature 68.0 - 752 °F
 13.0 µm/m-°C
@Temperature 20.0 - 800 °C
7.22 µin/in-°F
@Temperature 68.0 - 1470 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.5 %1.5 %
Chromium, Cr 12 %12 %
Iron, Fe 84 %84 %As Balance
Manganese, Mn 0.50 %0.50 %
Molybdenum, Mo 0.80 %0.80 %
Silicon, Si 0.30 %0.30 %
Vanadium, V 0.90 %0.90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm AISI D2 Cold Work Tool Steel
Crucible Steel AIRDI® 150 (AISI D2) Tool Steel
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 450°C

NCARN20 / 15859

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.