MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® G7705 GI-N (SEBS) Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form identified:
Kraton G7705 GI-N - supplied as a dense, natural color pellet

Region: North America; Asia Pacific; Europe; Japan; and South America

Applications: Compounding and Personal Hygiene; Adhesives, Sealant and Coatings; Bitumen Modification; Footwear; and Impact Modification

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 - 1.25 g/cc1.15 - 1.25 g/ccBAM 1014
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 39 - 4939 - 49BAM 1003
Tensile Strength 4.14 MPa600 psiASTM D412
 9.73 MPa1410 psiAfter Heat Aging 158 hrs at 150°C; ASTM D412
Elongation at Break 700 %700 %ASTM D412
 825 %825 %After Heat Aging 158 hrs at 150°C; ASTM D573
300% Modulus 2.07 MPa
@Strain 300 %
300 psi
@Strain 300 %
ASTM D412
Tear Strength 17.5 kN/m100 pliASTM D624
Compression Set  15 %
@Temperature 23.0 °C,
Time 79200 sec
15 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
 38 %
@Temperature 70.0 °C,
Time 79200 sec
38 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -63.0 °C-81.4 °FASTM D746
Flame Spread 50.8 mm/min2.00 in/minFVSS302/SAE J369 in/min
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 193 - 204 °C380 - 400 °F
Front Barrel Temperature 204 - 216 °C400 - 420 °F
Nozzle Temperature 420 - 450 °C788 - 842 °F
Mold Temperature 26.7 - 65.6 °C80.0 - 150 °F
Injection Pressure 3.45 - 4.83 MPa500 - 700 psi
Back Pressure 0.689 - 1.38 MPa100 - 200 psi
 
Descriptive Properties
Ozone ResistanceNo cracking100 pphm, 72 hr, 38°C, ASTM D518/1149

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® G7705 GI-B (SEBS) Compound
Avient Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE)
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® G2705 GU (SEBS) Compound
Kraton® G1641 H (SEBS) Linear Triblock Copolymer

PKRA9916 / 132816

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.