MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Edinburg Plastics DGG694 PA 6/6 Heat Stabilized, 43% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Appearance: General Purpose Colors

Processing Methods: Injection

Applications: Glass Filled

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D792-91
Linear Mold Shrinkage 0.00010 - 0.0030 cm/cm0.00010 - 0.0030 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 221 MPa32000 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Yield Strength 303 MPa44000 psiASTM D790
Flexural Modulus 11.0 GPa1600 ksiASTM D790
Izod Impact, Notched 1.44 J/cm2.70 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 252 °C486 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 288 - 299 °C550 - 570 °F
Middle Barrel Temperature 277 - 288 °C531 - 550 °F
Front Barrel Temperature 282 - 288 °C540 - 550 °F
Nozzle Temperature 282 - 288 °C540 - 550 °F
Melt Temperature 288 °C550 °F
Mold Temperature 60.0 - 99.0 °C140 - 210 °F
Drying Temperature 82.0 °C180 °F
Dry Time 4.00 - 24.0 hour4.00 - 24.0 hour
Moisture Content <= 0.20 %<= 0.20 %
Dew Point >= -17.8 °C>= 0.000 °F
Back Pressure 0.276 - 0.689 MPa40.0 - 100 psiLower is better
Screw Speed 30 - 70 rpm30 - 70 rpmLower is better

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Celanese Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced
Celanese Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Clariant Renol 66G15BL-195 Blue Nylon 66, 15% Glass Fiber Reinforced
Celanese Nilit FRIANYL C73 MG40 Nylon 6.6/6 for injection molding, 40% mineral filled

PEDIN022 / 183525

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.