MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Texin® 990 R Thermoplastic Polyurethanes (TPU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Texin 990R resin is a polyether-based thermoplastic polyurethane with a Shore hardness of approximately 90A. It contains an internal mold release additive. This resin can be processed by injection molding or extrusion.

Properties / Applications: Texin 990R resin offers outstanding abrasion resistance, impact strength, toughness, and flexibility. It also exhibits excellent hydrolytic stability, and exceptional mold release characteristics. Texin 990R natural color resin complies with FDA food-contact regulations 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber Articles Intended for Repeated Use), subject to the limitations of these and any other applicable regulations. It is also listed under NSF Standard 61 for use in potable water applications. Typical applications include belting, hose, seals and gaskets, tubing, cable jackets, hose jackets, athletic soles, casters, film, extruded profiles, and miscellaneous molded articles.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 2.54 mm
0.0080 in/in
@Thickness 0.100 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.54 mm
0.0080 in/in
@Thickness 0.100 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
Tensile Strength at Break 41.4 MPa6000 psiASTM D412
Tensile Stress at Strain  6.90 MPa
@Strain 50 %
1000 psi
@Strain 50 %
ASTM D412
 7.65 MPa
@Strain 100 %
1110 psi
@Strain 100 %
ASTM D412
 14.5 MPa
@Strain 300 %
2100 psi
@Strain 300 %
ASTM D412
Elongation at Break 520 %520 %ASTM D412
Flexural Modulus 0.0414 GPa6.00 ksiASTM D790
Compressive Strength 0.700 MPa102 psi2% Deflection; ASTM D 575
 1.70 MPa247 psi5% Deflection; ASTM D 575
 3.10 MPa450 psi10% Deflection; ASTM D 575
 4.50 MPa653 psi15% Deflection; ASTM D 575
 5.90 MPa856 psi20% Deflection; ASTM D 575
 7.20 MPa1040 psi25% Deflection; ASTM D 575
 19.3 MPa2800 psi50% Deflection; ASTM D 575
Resilience 4040[%], Bayshore; ASTM D2632
Tear Strength 96.3 kN/m549 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 25
@Load 1.00 kg
25
@Load 2.20 lb
[mg] Loss, H-18; ASTM D3489
Compression Set  13 %
@Temperature 23.0 °C,
Time 79200 sec
13 %
@Temperature 73.4 °F,
Time 22.0 hour
postcured; ASTM D395-B
 20 %
@Temperature 23.0 °C,
Time 79200 sec
20 %
@Temperature 73.4 °F,
Time 22.0 hour
as molded; ASTM D395-B
 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
postcured; ASTM D395-B
 75 %
@Temperature 70.0 °C,
Time 79200 sec
75 %
@Temperature 158 °F,
Time 22.0 hour
as molded; ASTM D395-B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 106 °C223 °FRate A; ASTM D1525
Brittleness Temperature >= -55.6 °C>= -68.0 °FASTM D746
Glass Transition Temp, Tg -44.0 °C-47.2 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 199 °C360 - 390 °FInjection
Middle Barrel Temperature 182 - 204 °C360 - 399 °FInjection
Front Barrel Temperature 182 - 210 °C360 - 410 °FInjection
Nozzle Temperature 188 - 213 °C370 - 415 °FInjection
Zone 1 182 - 199 °C360 - 390 °FExtrusion
Zone 2 193 - 210 °C379 - 410 °FExtrusion
Zone 3 193 - 216 °C379 - 421 °FExtrusion
Die Temperature 193 - 216 °C379 - 421 °FExtrusion
Melt Temperature 202 °C396 °FInjection
 202 °C396 °FExtrusion
Mold Temperature 16.0 - 43.0 °C60.8 - 109 °FInjection
Injection Pressure 34.5 - 68.9 MPa5000 - 10000 psi2nd stage
 41.4 - 96.5 MPa6000 - 14000 psi1st stage
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 990 Thermoplastic Polyurethanes (TPU)
Huntsman IROGRAN® A 95 K 4977 TPU-High Temperature Performance
Ineos Nova 1300 High Heat Crystal Polystyrene
Covestro Texin® 288 Thermoplastic Polyurethanes (TPU)
Covestro Texin® 945U Urethane Thermoplastic Elastomer

PCOVEST0987 / 202770

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.