MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kuraray Genestar™ G1350H Nylon, 35% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in a wide range of electrical and electronics components as UL94 HB flammability rating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/cc
Water Absorption 1.4 %1.4 %
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
Melt Flow 42 g/10 min
@Load 2.16 kg,
Temperature 320 °C
42 g/10 min
@Load 4.76 lb,
Temperature 608 °F
ASTM D1238
Spiral Flow 5.30 cm
@Load 750 kg,
Temperature 320 °C
2.09 in
@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.0 MPa6530 psiWeld; ASTM D638
 180 MPa26100 psiASTM D638
Elongation at Yield 0.60 %0.60 %Weld; ASTM D638
 4.0 %4.0 %ASTM D638
Flexural Strength 230 MPa33400 psiASTM D790
Flexural Modulus 10.0 GPa1450 ksiASTM D790
Izod Impact, Notched 1.15 J/cm2.15 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.4
@Frequency 1e+10 Hz
3.4
@Frequency 1e+10 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm762 kV/inASTM D149
Dielectric Loss Index 0.0090
@Frequency 1e+10 Hz
0.0090
@Frequency 1e+10 Hz
ASTM D150
Comparative Tracking Index >= 600 V>= 600 VASTM UL746A
 
Thermal PropertiesMetricEnglishComments
Melting Point 306 °C583 °F
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FASTM D648
Glass Transition Temp, Tg 125 °C257 °F
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kuraray Genestar™ G1350A-M42 Nylon, 35% Glass Filled
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled
LNP Lexan® EXCP0076 Polycarbonate, 30% Glass Fiber Reinforcement

PKUR117 / 162506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.