MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow PAPI™ 27 Polymeric MDI
Categories: Fluid; Polymer

Material Notes: PAPI™ 27 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a narrow molecular weight distribution and a high reactivity. Applicable to many foam processes, this product is compatible with rigid polyether and polyester polyols, making it suitable for a full range of low- to high-density semi-rigid foams, rigid foams and structural RIM processing.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Viscosity 150 - 220 cP150 - 220 cP
Viscosity Measurement 5.0 - 105.0 - 10[cps/mo.] Viscosity growth
Molecular Weight 340 g/mol340 g/mol
Vapor Pressure <= 1.30e-8 bar<= 0.00000975 torr
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.0170.017HCl content, %
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1170 µm/m-°C
@Temperature 20.0 °C
650 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.80 J/g-°C0.430 BTU/lb-°F
Thermal Conductivity 0.126 W/m-K0.870 BTU-in/hr-ft²-°F
Boiling Point 330 °C626 °F
Decomposition Temperature 230 °C446 °F
Flash Point >= 204 °C>= 400 °FASTM D93 Closed Cup
 
Descriptive Properties
NCO Content %31.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow PAPI™ 94 Polymeric MDI
Covestro DESMODURE® N 3600 Polyurethane
Dow PAPI™ 20 Polymeric MDI
Dow BETAFOAM™ 87100 MDI & PMDI Isocyanate
Dow BETAMATE™ 7200 Polyurethane Prepolymer

PDOW1398 / 30616

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.