MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aleris Weldural Aluminum Alloy, 100 mm Thickness
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Sample treatment not specified for property data.

Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldability and machinability. Fair corrosion resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.84 g/cc0.103 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 130130
Hardness, Knoop 163163Estimated from Brinell
Hardness, Rockwell A 49.449.4Estimated from Brinell
Hardness, Rockwell B 7979Estimated from Brinell
Hardness, Vickers 149149Estimated from Brinell
Tensile Strength, Ultimate >= 415 MPa>= 60200 psiMinimum
 455 MPa66000 psiTypical
 105 MPa
@Temperature 300 °C
15200 psi
@Temperature 572 °F
Typical, after 10,000 hours
 185 MPa
@Temperature 250 °C
26800 psi
@Temperature 482 °F
Typical, after 10,000 hours
 240 MPa
@Temperature 200 °C
34800 psi
@Temperature 392 °F
Typical, after 10,000 hours
 320 MPa
@Temperature 150 °C
46400 psi
@Temperature 302 °F
Typical, after 10,000 hours
 380 MPa
@Temperature 100 °C
55100 psi
@Temperature 212 °F
Typical, after 10,000 hours
Tensile Strength, Yield  >= 305 MPa
@Strain 0.2 %
>= 44200 psi
@Strain 0.2 %
Minimum
 350 MPa
@Strain 0.2 %
50800 psi
@Strain 0.2 %
Typical
Elongation at Break >= 5.0 %>= 5.0 %Minimum
 7.5 %7.5 %Typical
Modulus of Elasticity 73.8 GPa10700 ksi
Machinability 70 %70 %
Shear Strength 267 MPa38700 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000590 ohm-cm0.00000590 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.5 µm/m-°C
@Temperature 20.0 - 100 °C
12.5 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 130 W/m-K902 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 93 %93 %
Copper, Cu 5.8 - 6.8 %5.8 - 6.8 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg <= 0.10 %<= 0.10 %
Manganese, Mn 0.20 - 0.40 %0.20 - 0.40 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.30 %<= 0.30 %
Titanium, Ti 0.020 - 0.10 %0.020 - 0.10 %
Zinc, Zn <= 0.10 %<= 0.10 %
Zirconium, Zr 0.10 - 0.25 %0.10 - 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Aleris Hokotol Aluminum Alloy, 100 mm Thickness
China Tungsten NT3 Titanium Carbonitride Alloy
Overview of materials for 2000 Series Aluminum Alloy
Aluminum 2011-T3

NHOOG20 / 17347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.